PID;Reagent;Formula;MW;CAS;EU;Hazard Class;UN/NA;Packing group;DG weight (Kg);MSDS;Hydroscopic;Appearance;Typical uses;Special notes for package label AL;Aluminium powder (medium fine);Al;27;7429-90-5;231-072-3;4.3;UN1396;II;;Yes;No;Grey fine metallic dry powder.;Reducing agent. Hydrogen gas production.;Product will decompose if exposed to moisture. ALCL;Aluminium chloride (hexahydrate);AlCl3.6H2O;241.4;7784-13-6;Unlisted;8;UN1726;II;;Yes;Yes;White crystalline solid.;Soluble aluminium salt for aqueous reactions.; AMAC;Ammonium acetate;NH4CO2CH3;77.1;631-61-8;211-162-9;Not regulated;;;;Yes;Yes;Clumpy translucent crystalline solid.;Buffer solutions. Analytical chemistry.;Repackage once opened in a sealed air-tight container. AMCL;Ammonium chloride;NH4Cl;53.5;12125-02-9;235-186-4;9.2;UN9085;III;230;Yes;No;White crystalline solid.;Sublimation demonstration. Ammonia gas source.; AMMO;Ammonium heptamolybdate (tetrahydrate);(NH4)24Mo7O24.4H2O;1163.9;12027-67-7;234-320-9;Not regulated;;;;Yes;No;White crystalline solid.;Analytical chemistry. Froehde reagent.; AMPS;Ammonium perdisulfate;(NH4)2S2O8;228.2;7727-54-0;231-786-5;5.1;UN1444;III;;Yes;No;White crystalline solid.;General purpose oxidising agent. Radical reactions.; BAHY;Barium hydroxide (anhydrous);Ba(OH)2;171.3;17194-00-2;241-234-5;8;UN3262;II;;Yes;Yes;Fine white dry powder.;Source of barium salts.; BENZA;Benzoic acid (anhydrous);C6H5COOH;122.1;65-85-0;200-618-2;9.2;UN9094;III;230;Yes;No;Fine white crystalline solid.;Recrystallisation demonstration.; BORA;Boric acid;H3BO3;61.8;10043-35-3;233-139-2;Not regulated;;;;Yes;No;Fine white dry powder.;Buffer solutions. Analytical chemistry.;Grade is not suitable for food / health usage. CAHY;Calcium hydroxide;Ca(OH)2;74.1;1305-62-0;215-137-3;8;UN3262;III;;Yes;Yes;Fine white dry powder.;General purpose alkali. Source of calcium salts.; PHPA;pH paper (1-14) strips;;;;;Not regulated;;;;No;No;Small paper booklet.;Testing acidity / alkalinity of solutions.; CUSUA;Copper sulfate (anhydrous);CuSO4;159.6;7758-98-7;231-847-6;9;UN3077;III;;Yes;Yes;Light grey dry fine powder.;Source of copper compounds.; CUSU;Copper sulfate (pentahydrate);CuSO4.5H2O;249.7;7758-99-8;231-847-6;9;UN3077;III;;Yes;No;Blue crystalline solid.;Source of copper compounds.; GLYC;Glycine;NH2CH2COOH;75.1;56-40-6;200-272-2;Not regulated;;;;Yes;No;Fine white dry powder.;Demonstration of amino acid solubility.;Grade is not suitable for food / health usage. HEXAM;Hexamine;C6H12N4;140.2;100-97-0;202-905-8;4.1;UN1328;III;;Yes;No;White crystalline solid.;Nitrogen / ammonia source.; HYXCL;Hydroxylamine hydrochloride;NH2OH.HCl;69.5;5470-11-1;226-798-2;8;UN2923;III;;Yes;Yes;White crystalline solid.;Preparation of oximes. Nitrous oxide source.; FE;Iron metal powder (reduced);Fe;55.8;7439-89-6;231-096-4;4.1;UN3089;III;;Yes;No;Dark grey metallic dry powder.;Reducing agent.;Product will decompose if exposed to moisture. FE2SU;Iron (II) sulfate (heptahydrate);FeSO4.7H2O;278;7782-63-0;231-753-5;9.2;UN9125;III;50;Yes;No;Green-grey crystalline solid.;Source of iron (II) compounds. Analytical chemistry.; LIHY;Lithium hydroxide;LiOH;24;1310-65-2;;;UN2680;II;1;Yes;Yes;White microcrystalline solid.;Source of lithium compounds.;Repackage once opened in a sealed air-tight container. MG;Magnesium metal turnings;Mg;24.3;7439-95-4;231-104-6;4.1;UN1869;III;;Yes;No;Metallic shavings.;Reducing agent.; MGSU;Magnesium sulfate (pentahydrate);MgSO4.5H2O;210.4;15553-21-6;;9;UN3077;III;;Yes;No;White crystalline solid.;Source of magnesium salts.;Grade is not suitable for food / health usage. MNSU;Manganese sulfate (monohydrate);MnSO4.H2O;169;10034-96-5;232-089-9;9;UN3077;III;;Yes;No;Pale pink crystalline solid.;Source of manganese salts and manganese dioxide.; NICA;Nickel carbonate (basic);NiCO3.2Ni(OH)2.4H2O;376.2;12607-70-4;222-068-2;9;UN3077;III;5;Yes;No;Fine green dry powder.;Source of nickel salts.; OXALA;Oxalic acid (dihydrate);(COOH)2;126.1;6153-56-6;612-167-2;8;UN3261;II;;Yes;No;White crystalline solid.;Mild reducing agent.; PHTHAN;Phthalic anhydride;C6H4(CO)2O;148.1;85-44-9;201-607-5;8;UN2214;III;;Yes;Yes;Fine white dry powder with small lumps.;Source of phthalates. Synthesis of luminol dye.; KCA;Potassium carbonate (anhydrous);K2CO3;138.2;584-08-7;209-529-3;Not regulated;;;;Yes;Yes;Fine white dry powder.;Dessicant. Source of potassium salts.;Repackage once opened in a sealed air-tight container. KCHR;Potassium chromate;K2CrO4;194.2;7789-00-6;232-140-5;5.1;UN1479;II;4;Yes;No;Yellow crystalline solid.;Safer alternative oxidising agent to dichromate.; KFE2CY;Potassium hexocyanoferrate (II) (trihydrate);K4Fe(CN)6.3H2O;422.4;14459-95-1;237-323-3;Not regulated;;;;Yes;No;Yellow crystalline solid.;Prussian blue dye. Analytical chemistry. Anti-caking agent.;Grade is not suitable for food / health usage. KIODA;Potassium iodate;KIO3;214;7758-5-6;231-831-9;5.1;UN1479;II;;Yes;No;White crystalline solid.;Analytical chemistry.;Grade is not suitable for food / health usage. KI;Potassium iodide;KI;166;7681-11-0;231-659-4;Not regulated;;;;Yes;No;White crystalline solid.;Titration of oxidising agents such as bleach.;Grade is not suitable for food / health usage. KPERM;Potassium permanganate;KMnO4;158;7722-64-7;231-760-3;5.1;UN1490;II;;Yes;No;Black-purple crystalline solid.;General purpose oxidising agent.; SALICA;Salicylic acid;C6H4OHCOOH;138.1;69-72-7;200-712-3;Not regulated;;;;Yes;No;Fine white crystalline solid.;Preparation of aspirin and oil of wintergreen.;Grade is not suitable for food / health usage. NAAC;Sodium acetate (anhydrous);NaCO2CH3;82;127-09-3;204-823-8;Not regulated;;;;Yes;Yes;Fine white dry powder.;Preparation of acetic acid.; NABEN;Sodium benzoate;C6H5COONa;144.1;532-32-1;208-534-8;Not regulated;;;;Yes;No;Fine white dry powder.;Preservative. Source of benzoic acid.;Grade is not suitable for food / health usage. NAHSI;Sodium bisulfite;NaHSO3;104.1;7631-90-5 ;231-548-0 ;8;UN3260;III;;Yes;No;Fine white dry powder.;Demonstration of ketone adduct formation.;Grade is not suitable for food / health usage. NACA;Sodium carbonate (anhydrous);Na2CO3;106;497-19-8;207-838-8;Not regulated;;;;Yes;Yes;Fine white dry powder.;Dessicant. Source of sodium salts.;Repackage once opened in a sealed air-tight container. NANTA;Sodium nitrate;NaNO3;85;7631-99-4;231-554-3;5.1;UN1498;III;;Yes;Yes;White crystalline solid.;General purpose oxidising agent.; NANTI;Sodium nitrite;NaNO2;69;7632-00-0;231-555-9;5.1;UN1500;III;;Yes;No;Pale yellow crystalline solid.;Preservative and meat pickling. Source of nitrite.;Grade is not suitable for food / health usage. SULF;Sulfur powder;S;32.1;7704-34-9;231-722-6;4.1;UN1350;III;;Yes;No;Fine yellow dry powder.;Demonstration of burning and sulfur dioxide.;Grade is not suitable for food / health usage. THIUR;Thiourea;(NH2)2CS;76.1;62-56-6;200-543-5;6.1;UN2811;III;12;Yes;No;White crystalline solid.;Reaction catalyst. Source of sulfur for reactions.; SNCL;Tin (II) chloride (dihydrate);SnCl2.2H2O;225.6;10025-69-1;231-868-0;8;UN3260;III;;Yes;No;White crystalline solid.;General purpose reducing agent.; UREA;Urea;(NH2)2CO;60.1;57-13-6;200-315-5;Not regulated;;;;Yes;No;White crystalline solid.;Source of nitrogen and ammonia.; VANIL;Vanillin (food grade);C8H8O3;152.2;121-33-5;204-465-2;Not regulated;;;;Yes;No;Fine white dry powder.;Flavouring. Demonstrations of simple organic reactions.;Grade is suitable for food usage. ZN;Zinc metal powder;Zn;65.4;7440-66-6;231-175-3;4.3;UN1436;II;;Yes;No;Dark grey metallic lumpy powder.;General purpose reducing agent.;Repackage once opened in a sealed air-tight container.