toxicity might not be the problem
if you mind about the toxicity of NH3, i can only say i made huge amounts of NH3 outdoors in the gar ...
12-9-2002 at 15:45
by: Hoffmann-LaRoche
sounds like the holy grail for cheapskates
Na2SO4 could be replaced by K2SO4 in that reaction, i guess.
Then K2SO4 could be made out of calciu ...
12-9-2002 at 10:19
by: Hoffmann-LaRoche
Cheap H+ from ammoniumsulfate-fertilizer
You may right if u mention NH4HSO4 not really to be a strong acid....
Ive also thought of methods t ...
11-9-2002 at 13:45
by: Hoffmann-LaRoche
cant get no MOH, Vulture
thanks but i cant get methanol where i live.
Thats why i am fooling around with this stuff..

Gre ...
11-9-2002 at 13:34
by: Hoffmann-LaRoche
Cheap H+ from ammoniumsulfate-fertilizer
For those countries, H2SO4 is hard to get, or expensive, NH4HSO4 could be considered as working in m ...
11-9-2002 at 04:07
by: Hoffmann-LaRoche
sulfuric/hydrochloric acid replacement
For AP synth, also NaHSO4(drain cleaners) and also my cheap favourite, NH4HSO4 will probably work.
...
11-9-2002 at 03:51
by: Hoffmann-LaRoche
Pb(NO3)2
sorry for the misleading equations...i thought it would be obvious to you this process had to be don ...
10-9-2002 at 14:02
by: Hoffmann-LaRoche
formaldehyde from HCOOH?
thanks dude.....i´m confident one of these meths will work.....although some of them arent that che ...
10-9-2002 at 13:52
by: Hoffmann-LaRoche
Pb(NO3)2
ts ts, dont be that annoyed.
u would have to remove the caso4 by first diluting with water and filt ...
10-9-2002 at 12:25
by: Hoffmann-LaRoche
thats the cheapest method i can think of:
this process is unbeatable cheap as not even sulfuric acid is needed:

Ive successfully tested thi ...
10-9-2002 at 12:13
by: Hoffmann-LaRoche
Pb(NO3)2
Two easy (and very cheap) ways to lead nitrate(and huge amounts of NOx hehe):

1)H2SO4 + Ca(NO3)2 ...
10-9-2002 at 05:59
by: Hoffmann-LaRoche
methanol from CO2
I recently tried this process, which describes the conversion of CO2 into methanol, utilizing an ele ...
10-9-2002 at 05:34
by: Hoffmann-LaRoche
magnesium perchlorate for dehydration?
what about using magnesium perchlorate?
its used in place of P2O5( but much easier to prepare...

...
10-9-2002 at 05:19
by: Hoffmann-LaRoche
formaldehyde from HCOOH?
ive recently thought of making formaldehyde by reducing HCOOH or oxalic acid with nascent hydrogen.
...
10-9-2002 at 04:56
by: Hoffmann-LaRoche

  Go To Top