Aerosolized Zinc Found
Perhaps wash with acetone than ethanol? May remove some organics.
7-5-2008 at 11:57
by: chemkid
Drying Machine Ball Mill Anyone?
If i ever finish with all this damn school stuff I'll try this out with aluminum turnings to powder ...
24-4-2008 at 15:26
by: chemkid
Drying Machine Ball Mill Anyone?
Meant to say dryer. Converting the entire drying machine would be interesting. I was originally usin ...
23-4-2008 at 16:00
by: chemkid
Drying Machine Ball Mill Anyone?
So i had this idea last night...

Why not, rather than going through all the trouble of building a ...
23-4-2008 at 15:01
by: chemkid
Home Chemistry Society
Perhaps it would be more useful to list the reagents needed next to the reagent synthesized. Also if ...
19-4-2008 at 09:15
by: chemkid
Home Chemistry Society
I think we should change our reagent lists format. Its just going to be a pain to rewrite the OTC so ...
19-4-2008 at 08:58
by: chemkid
Home Chemistry Society
I guess it was just that day, because now the site is working just fine. Next question: Does anyone ...
11-4-2008 at 13:12
by: chemkid
Amateur/Home Chemistry: Historical Achievements
David Hahn is both a great failure and wonderful success of home chemistry. Leaning towards great fa ...
10-4-2008 at 15:44
by: chemkid
Home Chemistry Society
Does anyone else find the HCS page to be very slow? Sciencemadness and most other websites open quic ...
10-4-2008 at 11:08
by: chemkid
worst stench
I have heard the hydrogen sulfide has the lowest scent threshhold.
9-4-2008 at 12:55
by: chemkid
Concentrating DIlute Ammonia
I have no condenser, but perhaps i could use a flask to heat dilute ammonia, and then run a tube in ...
9-4-2008 at 11:49
by: chemkid
Concentrating DIlute Ammonia
I need some concentrated (30%) ammonia. I can by it of course online, but i have a few liters of per ...
8-4-2008 at 12:31
by: chemkid
Home Chemistry Society
Yay, i think i just created the first new page! A link to Other's Pages on the home page. Listing wh ...
8-4-2008 at 11:58
by: chemkid
Microscope photography
I have had success simply using a digital camera. I just place the lens against the lens of the micr ...
31-3-2008 at 11:17
by: chemkid
Copper(II) Aspirinate Synthesis
At the bottom 'Basic Recipe' it says to use KHCO3 (pottasium bicarbonate) could NaCO3 (sodium carbon ...
28-3-2008 at 08:38
by: chemkid
Synth help for a "Plastic"
I read that that required strong ammonia. Does anyone know if it can be done using a weak ammonia so ...
28-3-2008 at 05:02
by: chemkid
Home Chemistry Society
I'd saywe keep sciencemadness.org as an official part as the ACS if polverone would let us and then ...
18-3-2008 at 15:32
by: chemkid
Home Science logo competition!
I liked the logo woelen!
18-3-2008 at 15:22
by: chemkid
Green Filter Paper - Chromium, copper, iron, something else?
I treated the filterpaper with ammonia today. Dilute actually. Whatever it was it appears to have di ...
18-3-2008 at 12:08
by: chemkid
Basic preparative chemistry references
Try the library of this website
17-3-2008 at 15:25
by: chemkid
Green Filter Paper - Chromium, copper, iron, something else?
I honestly think i get stupider every day, I can't find the edit function now, whatever. Smaller ima ...
14-3-2008 at 18:59
by: chemkid
safe easy experiment
Whats unsafe about a controlled burn? What makes them cool is that they APPEAR unsafe ;) Boric acid ...
13-3-2008 at 16:22
by: chemkid
Green Filter Paper - Chromium, copper, iron, something else?
I dissolved an aluminum alloy (actually aluminum rivets) in HCl and left for several days. The solut ...
13-3-2008 at 16:19
by: chemkid
my chemistry site
Personally, from my own website making experiences, i have found it more effective to try to get as ...
13-3-2008 at 15:31
by: chemkid
Woo hoo, I built a working ball mill!!!
I have read a lot about ball mills now, and made one of my own. I have a bunch of aluminum turnings ...
10-3-2008 at 17:23
by: chemkid