DCM shrinks genuine coke bottle.
Yea, I have no photos, but it makes PET stretchy and soft, but strong enough to hold bottles form.
26-10-2019 at 03:04
by: TheMrbunGee
PTFE filters? What are they for?
I accidentally ordered MCE (mixed cellulose ester) filter papers, cut out and everything, sadly they ...
21-10-2019 at 11:44
by: TheMrbunGee
Would square filter housing work instead of round ones?
They would be harder to clean and uneven stresses might cause problems to material at certain pressu ...
18-10-2019 at 04:17
by: TheMrbunGee
"Firewire" E-Initiator
have not seen anything like that, picture in link does look like simple e-match, the plastic is prot ...
13-10-2019 at 09:47
by: TheMrbunGee
Brand new JJ-1 Over Head Laboratory Mixer speed cntrol not working... Help diagnosing problem please?
Sorry to read this!

So you are saying that everything works besides the speed control, so does i ...
12-10-2019 at 15:31
by: TheMrbunGee
"Firewire" E-Initiator
[rquote=624255&tid=154159&author=VSEPR_VOID]Has anyone ever heard of these? They claim to be ...
12-10-2019 at 10:49
by: TheMrbunGee
Buchner funnel
Today I confirmed, that round things like nice 70 ml ground glass joint buchner funnel do actually r ...
10-10-2019 at 10:25
by: TheMrbunGee
A new type of discussion board
Good luck!
9-10-2019 at 22:18
by: TheMrbunGee
Processing lead from batteries - finding a method that works
[rquote=623564&tid=154081&author=Praxichys]You probably already know this but lead ingots on ...
25-9-2019 at 11:09
by: TheMrbunGee
Deschem
I have ordered from deschem 5 times and not a single complaint. Glassware seems okay quality (I have ...
23-9-2019 at 05:19
by: TheMrbunGee
Synthesize ethylene glycol diacetate?
[rquote=622998&tid=153970&author=DavidJR]24% acetic acid is definitely not going to cut it f ...
16-9-2019 at 09:57
by: TheMrbunGee
Chemistry Diamonds on YouTube
[rquote=622945&tid=66255&author=j_sum1]I just came across Chemical Force https://www.youtube ...
15-9-2019 at 22:31
by: TheMrbunGee
DMT extraction.
"Reflux" times are overkill, NaOH amount is overkill (actually amounts all seem quite high). You hav ...
5-9-2019 at 08:19
by: TheMrbunGee
Safe preparation of lead oxides
On the right is purchased, yes and on the left is my attempt of melting lead metal and NaNO3, but I ...
26-8-2019 at 21:47
by: TheMrbunGee
Colorimetric powder identification?
Hey SM!

I got a box of different colorimetric powders, and because of some pretty color changes I ...
26-8-2019 at 01:01
by: TheMrbunGee
Safe preparation of lead oxides
You can make them at lower temperatures by melting lead with K/Na nitrate (not sure about other nitr ...
25-8-2019 at 20:06
by: TheMrbunGee
how to syntetize chloroacetone?



I am actually exited for these reactions, can other substances be halogenated by this process? ...
23-8-2019 at 17:36
by: TheMrbunGee
how to syntetize chloroacetone?
Few years ago I dissolved some copper bromide in acetone, it become clear and lachrymatory, I think ...
23-8-2019 at 04:13
by: TheMrbunGee
1952 soviet dentist amalgam composition
the text is all instructions on use for filling cavities, but it is called "copper amalgam" ,so I su ...
12-8-2019 at 06:59
by: TheMrbunGee
Buying chemicals in Poland "OTC"
[rquote=619991&tid=152908&author=mackolol]I'm from Poland and i can recommend you companies ...
8-8-2019 at 22:49
by: TheMrbunGee
Copper Acetate
Copper acetate grows most beautiful crystals I have seen, If you end up not doing anything with it, ...
8-8-2019 at 22:34
by: TheMrbunGee
Organic synthesis
If you want to make drugs, then you should learn to do so, step by step, on your own, until you lear ...
7-8-2019 at 14:14
by: TheMrbunGee
Sintered Funnel Clogged with Cr2O3
[rquote=619925&tid=152870&author=ZetekitoxinAB]Maybe try adding dropwise conc NaOH and 30% H ...
7-8-2019 at 14:06
by: TheMrbunGee
Water Pump
Really cheap power supplies on ebay [url=https://www.ebay.com/itm/AC-110V-220V-TO-DC-5V-12V-24V-Swit ...
23-7-2019 at 06:06
by: TheMrbunGee
KBr on ebayuk £15 for 1kg
[rquote=612729&tid=150170&author=fusso][rquote=612707&tid=150170&author=wg48temp9]re ...
16-5-2019 at 13:19
by: TheMrbunGee