Hydrogen Peroxide Production
hi,
i have various information about H2O2 Production but these patent has no instruction for making ...
24-8-2008 at 00:48
by: Fashist
Trinitrotoluene preparation
[quote][i]Originally posted by CD-ROM-LAUFWERK[/i]
my TNT did melt around 81°C, wich is pure
the ...
15-3-2008 at 05:05
by: Fashist
Trinitrotoluene preparation
Its true.
Merck Trifluoromethanesulfonic acid is 56 eur per liter.
1-3-2008 at 01:26
by: Fashist
Trinitrotoluene preparation
I Found Interesting Patent
http://www.freepatentsonline.com/WO2005005342.html
Nitric Acid+Trifluor ...
1-3-2008 at 01:01
by: Fashist
Acetic anhydride preparation
Merck SICL4 is 56$ per liter(cheap than Alfa)
If you order drum(190kg) it will be cheaper.
29-2-2008 at 00:50
by: Fashist
starch Problem!
Mr spark i didnt find that here(no chmical strore dont know what is that)
24-2-2008 at 13:49
by: Fashist
starch Problem!
thanks mr not important
gluco-amylase seems be better.
anybody know company that sale it?
thx

[E ...
24-2-2008 at 11:34
by: Fashist
starch Problem!
spit into my starch?
sure i search it before and i didnt find.
24-2-2008 at 07:09
by: Fashist
starch Problem!
Thanks of you
Mr sauron tapioca is commonly plant?(may i find that?)
Mr evil gluco-amylase is comm ...
24-2-2008 at 06:48
by: Fashist
starch Problem!
Thanks
I search it before but most of patent use plant like Cassava and koji kom and.. for hydrolyz ...
24-2-2008 at 03:45
by: Fashist
starch Problem!
i am looking for cheap component that broke starch to glucose
thx
24-2-2008 at 01:45
by: Fashist
Acetic anhydride preparation
Today i test the pyrosulphate method but no result!
i mix 250gram k2s2o7 and 165gram acona and add ...
22-2-2008 at 13:57
by: Fashist
Acetic anhydride preparation
Mr sauron you think potassium pyrosulphate wont work?
K2S207+ACONA->AC2O+na2so4+k2so4?
or
NA2S ...
20-2-2008 at 01:24
by: Fashist
Acetic anhydride preparation
I will try
K2S207+ACONA->AC2O+na2so4+k2so4
i just find pottasium pyrosulphate(old merck product ...
19-2-2008 at 04:41
by: Fashist
Acetic anhydride preparation
Now i cant Product any acetic anhydrid because merck dont sale acetyle chloride.(germany cut its tra ...
19-2-2008 at 03:56
by: Fashist
Acetic anhydride preparation
i think this is not good method because pocl3 is very toxic.
anybody has experience with sodium pyr ...
18-2-2008 at 23:23
by: Fashist
Acetic anhydride preparation
6 PCl5 + P4O10 → 10 POCl3

"Phosphorus pentachloride also forms POCl3 by reaction with w ...
17-2-2008 at 20:55
by: Fashist
Acetic anhydride preparation
POCL3+4ACONA->2AC2O+3NACL+NAPO3
Good idea
any body has idea?
17-2-2008 at 10:22
by: Fashist
Trinitrotoluene preparation
My Suggestion is Using Con.Nitric Acid
I Made it Using Dry Mg(NO3)2 + HNO3(57%) and then Distil.
10-2-2008 at 12:03
by: Fashist
Trinitrotoluene preparation
I used this book Ratio
http://rapidshare.com/files/90231545/fmx.zip.html
8-2-2008 at 12:31
by: Fashist
Trinitrotoluene preparation
I made tnt very easy by reflux system(see below picture)
First i made Dnt and then made tnt in the ...
7-2-2008 at 22:46
by: Fashist
Method For Drying Mg(No3)2
I made Mg(no3)2 before(MGCO3+HNO3).
I made nitric acid from an+h2so4 before but i want to try this ...
1-2-2008 at 01:12
by: Fashist
Method For Drying Mg(No3)2
Any body Know Simple Method For Drying Mg(No3)2 ?
and Anybody know how we can increase the concentr ...
30-1-2008 at 03:48
by: Fashist
keten lamp
Mr Nicodem Soon I will Send Picture of My System.
You Said I Use .5 ml for Testing?
21-1-2008 at 09:30
by: Fashist
keten lamp
My System is Larger than Normal System and I Need to Use 50cc Aniline Per Test.
My Acetone Boiler i ...