HNO3 and HDPE issue HDPE container seems quite strong and tough but over time that should change, and transfering conc. ... |
1-9-2013 at 02:12 by: chemliner |
HNO3 and HDPE issue 25944 |
31-8-2013 at 11:47 by: chemliner |
HNO3 and HDPE issue I have aquired 10l of 60% HNO3. Acid came packed in HDPE bottle(original package) , which have chang ... |