Thoughts On Anodes
Dann2, thanks for welcome.
Pictured anodes are RuO based and electrode is designed to generate low ...
26-10-2008 at 14:20
by: simple
Thoughts On Anodes
Here is corrosion caused by shunt current. You can see how the edge of the place was "chewed".

E ...
24-10-2008 at 21:39
by: simple
Thoughts On Anodes
Trying to load the image
24-10-2008 at 21:38
by: simple
Thoughts On Anodes
Hi Dann2,
'shunt current' is a leaking current between oppositely charged parts. Normally starts t ...
24-10-2008 at 21:31
by: simple
Thoughts On Anodes
Thinks to consider with Ti electrode design:
poor thermal conductivity
poor electrical conductivit ...
24-10-2008 at 18:59
by: simple
NaClO4 production using a Pt clad Ti anode and a Ti cathode.
axehandle , I have only partially read and understand what you are trying to do, but just want to co ...
14-11-2006 at 15:55
by: simple
NaClO4 production using a Pt clad Ti anode and a Ti cathode.
[quote][i]Originally posted by SAM4CH[/i]
How can I make perchlorate from NaCl using pure platinum ...
14-11-2006 at 15:46
by: simple
Thoughts On Anodes
jpsmith123 , eSplash do not manufacture - they resell. They sourse from different suppliers.
There ...
30-7-2006 at 22:54
by: simple
Thoughts On Anodes
Mesh electrodes in salt water chlorination game been used for a long time.
From our point of view t ...
28-7-2006 at 01:45
by: simple
Thoughts On Anodes
Nice to see someone knows Beer!
Anyway, for non reverse electrode you can get good samples from num ...
26-7-2006 at 00:24
by: simple
Thoughts On Anodes
http://www.vchlorin.com/cell.htm I know them, however did not test the perfomance of there's cells ( ...
25-7-2006 at 22:42
by: simple
question about distilling water
Regarding static discharge - i would agree with Magpie
25-7-2006 at 21:24
by: simple
question about distilling water
Exacly! Suprases the hell out of you when you test and not familiar with the process. Water coming ...
25-7-2006 at 21:13
by: simple
question about distilling water
We have USA made vaccum destiler (capacity about 150 galon per hour), we also have normal boiling ty ...
25-7-2006 at 20:14
by: simple
Cell for high current electrolysis of water
[quote][i]Originally posted by not_important[/i]
Salt water will give you chlorine, no matter what ...
25-7-2006 at 19:35
by: simple
Thoughts On Anodes
We have tested anode materials from a lot of suppliers including India. We test to strict specs in c ...
25-7-2006 at 19:28
by: simple
Cell for high current electrolysis of water
From what i know you need 10+ VDC to deplite water efecently.
The good way is to use salty water( ...
25-7-2006 at 18:42
by: simple
Thoughts On Anodes
If you aim for HOCL the best bet is DSA type anode. DSA is a brand name not the type. Same like SONY ...