Search |
Magnetic Carbon? I think that's doable in my kiln, bricks are rated for 1260c and element is good for just over 1100c ... |
22-2-2018 at 10:14 by: tacromx |
Magnetic Carbon? Thank you Aga.
Ill try some bread in the kiln,any estimates as to temperature and time? |
22-2-2018 at 09:42 by: tacromx |
Magnetic Carbon? It's contamination i suspect, tried a small sample in hydrochloric acid, as you can see from the pic ... |
22-2-2018 at 08:26 by: tacromx |
Magnetic Carbon? @Melgar
I have the carbon in a 500ml borosilicate beaker, when i place a 10x10mm neodymium undern ... |
21-2-2018 at 17:10 by: tacromx |
Magnetic Carbon? @Morgan
Yes it was a metal container.
Guess ill have to invest in a graphite crucible to know ... |
21-2-2018 at 16:04 by: tacromx |
Magnetic Carbon? Since im mainly into battery research i needed a kiln for making activated carbons, so i made one. M ... |
21-2-2018 at 16:01 by: tacromx |
Magnetic Carbon? So the day before i cooked up some sugar and zinc chloride in a 1:1 ratio in de-ionized water, cooke ... |
21-2-2018 at 14:52 by: tacromx |