Quote: Originally posted by MineMan  | Hello fellow scientist!
I am working on an independent study for the University and I need to acquire spherical aluminum powder in the following size ranges... I can’t find
any suppliers other than China... which I do not completely trust, or US nano, which is around $.50 cents a gram. I need a kilogram or two of the
following sizes.
10um-15um
40-50um
100um
Any ideas? It cannot be flake, it must be spherical so milling is out of the question, as far as sieving... I believe it would take too long and I
would need to start with 3-5x the amount of material needed.
Where can I acquire these specific sizes? |
Hey MineMan. I get aluminum from Toyal that is of pretty high quality. They have flake atomized as well as spherical/spheroidal. http://www.toyala.com/cgi-bin/r.cgi/powders_spherical_aero.h...
A Spanisch colleague of mine gets powdered metals from a company I can't really remember the name of for sure...I thinks it is Jengo or Jango or
something. They are European. Hope this helps, Tchuess! |