Jacob K - 1-6-2021 at 18:32

Figure 2.png - 2.2MB

It is very easy for a home chemist to create beautiful and large crystals of sodium ferrioxalate using relatively simple and readily available chemicals, and they can use the sodium ferrioxalate to study the fascinating processes of photochemistry and create blueprints (https://en.wikipedia.org/wiki/Potassium_ferrioxalate). Thus, I would recommend this project for an experienced home chemist.

To make sodium ferrioxalate, I created a procedure inspired by the one described in https://en.wikipedia.org/wiki/Sodium_ferrioxalate. I first added an excess of baking soda to aqueous ferric chloride hexahydrate (I used 12.06 grams), and I filtered out the resulting precipitate. I then added the resulting ferric hydroxide precipitate to an excess of oxalic acid, and the ferric hydroxide dissolved in the oxalic acid, which made a rusty-brown solution. In a separate container, I made sodium oxalate by neutralizing aqueous oxalic acid with baking soda. I then mixed the ferric oxalate solution with a slight molar excess of the resulting sodium oxalate, and a bright emerald green solution of sodium ferrioxalate formed. I then evaporated this solution in a light-tight container, and I obtained 7.8 grams of sodium ferrioxalate in the form of large crystals (see Figure 1), and this corresponds to a 45% yield, assuming a product formula of Na3[Fe(C2O4)3].

The steps in this process can be described by the following simplified reactions:
Reaction 1: FeCl3 (aq)+3NaHCO3 (aq)-->Fe(OH)3 (s)+3NaCl (aq)+3CO2 (g)
Reaction 2: 2Fe(OH)3 (s)+3H2C2O4 (aq)-->Fe2(C2O4)3 (aq)+6H2O (l)
Reaction 3: Fe2(C2O4)3 (aq)+3Na2C2O4 (aq)-->2Na3[Fe(C2O4)3] (s)

While my procedure successfully yielded large and beautiful crystals of product, I think it should be optimized for time efficiency and yield. This can be done by adding the ferric chloride to 3 equivalents of aqueous oxalic acid, neutralizing the solution with 3 equivalents of sodium hydroxide or bicarbonate (or 1.5 equivalents of sodium carbonate), and then slowly evaporating the mixture to obtain large crystals (idea from https://reactionchamber.org/sodium-ferrioxalate-complex-crys...). Although the solution would contain sodium chloride (unlike in my procedure), the sodium ferrioxalate should crystalize out first. Furthermore, to improve yield after removing the large crystals, the solution can be fully evaporated, and the remaining sodium ferrioxalate can be recrystallized from its mixture with sodium chloride using minimal amounts of hot water. This procedure would be much less cumbersome than my procedure, since it can be done using a single container and with no filtration steps.

Figure 1.png - 2.5MB

To help validate my product, I left it out in direct sunlight (see Figure 2). My product appears to be very sensitive to direct sunlight, as it turns from transparent to translucent and then from translucent to opaque, and it turns from a light emerald green to a muddy brown. The muddy brown color is likely due to the formation of sodium ferrooxalate and possibly other iron (II) and/or iron (III) decomposition products (https://en.wikipedia.org/wiki/Potassium_ferrioxalate). The photochemistry involved in this photodegradation is fascinating, and I would recommend the following article for anyone interested: Chen, J.; Browne; W. R. Photochemistry of Iron Complexes. Coord. Chem. Rev. 2018, 374, 15–35.

Using just ferric chloride, baking soda, and oxalic acid, I was able to create sodium ferrioxalate and explore the phenomenon of photochemistry. I believe that a creative home chemist may be able to use this compound to estimate the power output of the sun or perform other interesting experiments that leverage the sodium ferrioxalate’s unique photochemistry.



scienceboi - 2-6-2021 at 14:08

Nice write up! I might do this myself now. Thanks for sharing

Jacob K - 2-6-2021 at 16:14

Quote: Originally posted by scienceboi  
Nice write up! I might do this myself now. Thanks for sharing


Sure thing! I'm glad you liked it.

mayko - 13-12-2021 at 18:12

I had fun with this one. Behold, the forbidden hard candy!

forbiddenHardCandy.jpg - 233kB


Junk, P. C., Bacsa, J., & Thomas, N. C. (2021). Growing a Display Crystal of Recycled Potassium Tris(oxalato)ferrate(III) Trihydrate. Journal of Chemical Education, 98(10), 3400–3404. https://doi.org/10.1021/acs.jchemed.1c00776

These folks saved ferrioxalate leftovers from years of student waste and grew an enormous high quality crystal by slow evaporation. Check out this chonkster:

ferrioxalate_chonkster.jpeg - 183kB


Lion850 - 18-12-2021 at 19:36