Quote: Originally posted by Deathunter88  | | Hydrocarbons vapors diffuse through HDPE pretty easily and also soften it over time. For hydrocarbons with a low vapor pressure (like terpentine,
kerosene, mineral spirits), you'll form a partial vacuum in the bottle as more vapor is lost than can be replaced by the vapor pressure of the liquid
itself. This, combined with the softened HDPE, will cause the bottle to collapse. |
Thanks for the great explanation, on that basis my products should still be fine and will store better in glass. |