Endymions explanation is correct. Just try the experiment with CS2 replaced by methanol in similar volume. As a first start that will do. Always first
try at test tube scale before scaling up!
Making the solution of boric acid is easy. Add a spatula full of boric acid to 5 ml of methanol and dissolve. Burn the liquid. If it burns with a deep
grass green flame then it is ok. |