Sciencemadness Discussion Board

dropping gold oui of ar solution

jc the gold hunter - 17-10-2014 at 14:42

i have 3 oz's of gold in ar i used urea to neutralize acid then smb to drop gold no gold dropped .can i use ether to seperate liquids then keep ether (top) layer of liquid add oxalic acid at 180 degrees to this then use sodium hydroxide to drop gold now?

cyanureeves - 17-10-2014 at 15:04

3 oz. of gold? hell i'd evaporate the aqua regia down to a crust first then add smb.i bet it's still to acidic.

pneumatician - 31-10-2014 at 18:22

what is the end of this history?

Bert - 31-10-2014 at 18:41

I would like to see your complete procedure...

Do you use recycled materials, or are you using ores as primary source?

Damn. 3 oz of Gold as raw materials, and you're askng US how to proceed. $3,000.00 US $'s of (potential) product?