acquiring thermostat oven for high temperature

Cloner - 11-8-2005 at 10:04

I need to get a small oven that can be set to a certain temperature, interval up to 700 celsuis or something like that.

Where does one obtain such ovens? It's for my work so cost is not that important though it shouldn't be ridiculous even so. And not room consuming, I'd prefer something small.

Pottery and ceramic ovens

Lambda - 11-8-2005 at 18:58

Pottery Cloner, pottery and ceramic ovens. This stuff is made for the general public, mass produced, and cheap. Not the kind of small scale markeded ripoff prices you would expect from the chem supplier. Just make sure you use a thermocopple element to measure the temperature.

Do you need schematics for a thermocopple thermostate to do your temperature regulation and/or measurements ?

[Edited on 12-8-2005 by Lambda]

Cloner - 12-8-2005 at 06:23

No, I'd rather have an oven which includes this. In fact, I want an oven which is like my cooking oven at home, only with an extended temperature range.