Now I know that if an oxidizing agent such as H2O2 or Nitric Acid is added to the mix, the Iron II Sulfate will be oxidized into Iron III Sulfate. But
does a solution of HCl, Iron II Sulfate, and Sulfuric Acid alone also result in a reaction into the ferric when heated strongly? Same question also
for Iron II Sulfate + Sulfuric and high heat.
|