| The minerals in the lake are distributed as follows: 55.4 percent chloride, 32 percent sodium, 6.6 percent sulfate, 3.2 percent magnesium and 2.6
percent potassium. The lake also contains smaller amounts of calcium, bromine, lithium, boron and other minerals.[\quote] |