Sciencemadness Discussion Board

unknown dye - german label

e.liska - 28-9-2017 at 13:05

Anyone can read and understand this? The powder has a dark brownish violet color.

IMG_20170928_230427.jpg - 1.5MB

DraconicAcid - 28-9-2017 at 13:34

Fellaucht grun? I know the last word means green....

e.liska - 28-9-2017 at 14:36

I cannot google anything like this or similar.

phlogiston - 28-9-2017 at 19:28

Malachit grün maybe? It would match "MG". I can't make much sense of the first word on the label though. It doesn't look like any German word I know and only resembles malachite a little bit.

[Edited on 29-9-2017 by phlogiston]

e.liska - 28-9-2017 at 23:34

But dry malachite green is green, isn't it? This looks more like violet.

VSEPR_VOID - 29-9-2017 at 01:52

Could you possibly make a solution of it for us?

e.liska - 29-9-2017 at 02:51

The solution in tap water (pH about 7.5) is strong green. It takes very little powder to make a lot of color. Addition of baking soda does not change the color. My vinegar is brown, but it does not seem to change the color either. What is strange, there is a very slight effervescence in plain tap water.

IMG_20170929_124424.jpg - 550kB

VSEPR_VOID - 29-9-2017 at 17:00

You could send it off to be tested with some sort of spectrometer

e.liska - 30-9-2017 at 05:43

Couldn´t the first three letters bee FCF? Not sure how to read the German handwriting.

Anyway, if I put the powder on a white surface and add some water in a way that the crystals are not immediately dissolved and tiny streams of colored water forms around individual crystals or their small groups, it can be seen that there are some completely different, brownish-yellow streams of water. So is it some mixture? Or is it possible that some crystals aged differently than others?

Texium - 30-9-2017 at 06:29

Hey, you may be onto something with the FCF. FCF Fast Green is a common dye, and the German name for it is FCF echtgrün!

If that's what they were trying to write though, they must have had really terrible handwriting.

[Edited on 9-30-2017 by zts16]

e.liska - 30-9-2017 at 09:26

So, the writing has been deciphered, it reads Sella Echt Grün GM, which is German for SELLA® Fast Green GM, which is some commercial dye for leather. The only information I was able to google up is this file https://www.tfl.com/pdocs/PIN/SELLA_Fast_Green_GM_PIN_GLO_EN...


"SELLA® Fast Green GM is a mixture of direct and acid dyes imparting a neutral to slightly yellowish green shade (grass green). It is especially suitable for green shades with very good fastness properties"

This explains the different colored crystals and maybe even the effervescence. But sadly I cannot google any detailed information about the chemical composition.

[Edited on 30-9-2017 by e.liska]

Morgan - 30-9-2017 at 20:52

Contains no metals.
http://www.saceasrl.it/schede/dyes//Global_dyes.pdf

gagepoon - 4-10-2017 at 00:57

It's Malachite green which is one of the basic dye used as a dyestuff and controversially as an antimicrobial in aquaculture. Malachite green is traditionally used as a dye for materials such as silk, leather, and paper. Sharing some sites to get more information on Malachite green dye.

En.wikipedia.org/wiki/Malachite_green
Dyespigments.net/basic-dyes-manufacturer-supplier-exporter-india.html
Ezinearticles.com/?Malachite---Mother-Natures-Finest&id=7487749

e.liska - 4-10-2017 at 04:05

Quote: Originally posted by gagepoon  
It's Malachite green...


What is your source? It does not look like a malachite green to me. Anyway, your link to the malachite mineral article is plainly wrong, because malachite green is not the same chemical as malachite mineral is.

e.liska - 4-10-2017 at 04:07

What we know so far:

- it is a mixture of at least two different dyes
- it does not contain metal
- its color is not dependent on pH in the vinegar to baking soda range

ZeLaboratorium - 4-10-2017 at 05:17

Add some stronger acids/bases

malachit green changes color at an Ph of 1.8 or 11.5 (wikipedia)

aga - 4-10-2017 at 06:03

"unknown dye" is basically what the label says.

Basically their spelling was poor - it should read "vielleicht grün MG" which translates nicely.

(how they spelt the word was phonetically very close)

e.liska - 4-10-2017 at 06:46

No, it is already deciphered as Sella Echt Grün GM (SELLA® Fast Green GM) - commercial dye of unknown composition.

unionised - 4-10-2017 at 07:16

So far, we seem to have clearly established that we don't know, with any certainty, what the stuff is.
Kudos (and welcome) to ZeLabatorium for actually proposing something that might help to find out.

e.liska,

do you have access to any stronger acids or bases?

e.liska - 4-10-2017 at 07:28

I have common household NaOH (granulate), but no strong acids. I have basically only a kitchen "lab".

[Edited on 4-10-2017 by e.liska]

unionised - 4-10-2017 at 12:34

Well, malachite green goes clear in sodium hydroxide solution.
If you can get some hydrochloric acid - sometimes sold as a cleaner for patios/ decking- you might be able to get it to turn yellow.

aga - 4-10-2017 at 13:46

Quote: Originally posted by e.liska  
No, it is already deciphered as Sella Echt Grün GM (SELLA® Fast Green GM) - commercial dye of unknown composition.

Say out loud what is written on that label in German, then try to work out what those sounds mean.

All Written language (apart from Maths and a few others) are a way to record audible noises that convey information.

I could easily be wrong, of course, and a single solution is always easier to deal with.

Hopefully you'll find something useful to do with the substance.

DraconicAcid - 5-10-2017 at 07:04

You could try paper chromatography on it to see if it really is a mixture.

e.liska - 8-10-2017 at 01:04

When I add several granules of NaOH to few milliliters of the green solution, the solution heats a lot (dissolving NaOH) but color does not change too much. I think the base does not change at all, but the solution looks differently because lots of small particles precipitate in it, so what I get is suspension of darker particles in green solution.

SWIM - 8-10-2017 at 10:17

Since it is a mixture of direct and acid dyes, maybe they can be partitioned to some extent with the right solvents.
Wouldn't the direct dyes be likely to have more affinity for some organic solvents than the acid dyes?








100PercentChemistry - 9-10-2017 at 14:29

https://www.zauba.com/import-sella+fast+green-hs-code.html


This website says that this dye is used in the leather industry.

I also found that it's in these paints(I know it's not very helpful).
http://www.fashiontrendsetter.com/downloads/TFL-SS2009-Trend...
http://www.vlgrupo.com/TENDENCIAS/primavera2010/VLGRUPO_livi...

[Edited on 10-9-2017 by 100PercentChemistry]

[Edited on 10-9-2017 by 100PercentChemistry]

[Edited on 10-9-2017 by 100PercentChemistry]

e.liska - 17-10-2017 at 14:47

So I have tried some chromatography. It is a mix. From left to right:

1. my first run - I used previously dissolved dye that was left in a glass after it dried out. I have addes some denatured ethanol and probably also some water, do not remember exactly. This one has the most focused bands in the front.

2. Another run with denatured alcohol only. The bands in front are not so nice.

3. Water only. No visible separation at all.

4. Water alcohol mix. Nice separation but not so nicely focused as in the first run.

IMG_20171017_235633.jpg - 407kB

[Edited on 17-10-2017 by e.liska]

e.liska - 20-10-2017 at 02:26

ethanol, run overnight - much better

How many different dyes it is?

IMG_20171018_085820.jpg - 155kB

DraconicAcid - 20-10-2017 at 07:39

Looks like at least three- a blue, a yellow, and a green. You can separate the dyes by cutting the paper, and see if any of them respond to different pH solutions.