kadriver - 4-1-2018 at 15:20
Here is a video that I created of an experiment that I did to recover silver from X-ray films:
https://youtu.be/0tn-a0S0FD8
kadriver
j_sum1 - 4-1-2018 at 16:43
I have been enjoying your work recently and will watch that vid soon.