Sciencemadness Discussion Board

Aerogel Production, amateur

dapper - 26-5-2007 at 19:12

Is the hardest part of making aerogels DIY the extraction of the water/alcohol from the sol-gel with supercritical CO2?

not_important - 26-5-2007 at 22:08

You don't need supercritical extraction, see US patents 5565142 and 5680713 for example.

JohnWW - 27-5-2007 at 13:56

An e-book on the subject of sol-gels has recently been added to the collection on www.gigapedia.org.

dapper - 30-5-2007 at 06:35

Much appreciation, thankyou.

Twospoons - 30-5-2007 at 18:33

Have you got a link? A search on gigapedia returned nothing.

aerogel catalyst materials

Rosco Bodine - 21-12-2007 at 04:05

Just ran across this while looking for something else ,
but thought it should be added here .

Attachment: Ambient Pressure Synthesis of Aerogel-Like Vanadium Oxide and Molybdenum Oxide.pdf (83kB)
This file has been downloaded 1902 times


DrP - 8-1-2008 at 08:29

So, has anyone here actually made Aerogels without supercritical CO2 yet? (I mean without them falling to bits).

Spargine - 13-1-2008 at 16:44

Actually, someone did. http://homepages.cae.wisc.edu/~aerogel/aboutaerogel.html

They even supercritically dried out jello, making an edible aerogel.

The_Davster - 13-1-2008 at 17:35

I like! I wonder if those are just standard steel pipe parts, or if they are high pressure rated?

DrP - 5-2-2008 at 01:21

Quote:
Originally posted by Spargine
Actually, someone did. http://homepages.cae.wisc.edu/~aerogel/aboutaerogel.html

They even supercritically dried out jello, making an edible aerogel.


Well 'they' used supercritical CO2 and are not members of this forum.

Aerogel garage syntheses

Mailinmypocket - 5-11-2012 at 18:17

Just came across these videos on YouTube. This guys whole channel is really amazing and he explains everything in detail- very ingenious guy!


Anyhow, making aerogel, video #1 and #2:

Silica aerogel

Supercritical methanol aerogel