[*] posted on 12-4-2006 at 18:27
Glassware quality question


I am interested in purchasing a distillation kit from UGT (United Glass Technologies). I do not know how their quality of glassware would fare against Pyrex/Kimax(kimble exax).
View user's profile View All Posts By User
MadHatter
International Hazard
*****




Posts: 1332
Registered: 9-7-2004
Location: Maine
Member Is Offline

Mood: Enjoying retirement

[*] posted on 12-4-2006 at 18:35
Bomex


Make sure it isn't Bomex and that it's one of the higher quality borosilicates(Kimax,Pyrex,
Simax,Schott-Duran).




From opening of NCIS New Orleans - It goes a BOOM ! BOOM ! BOOM ! MUHAHAHAHAHAHAHA !
View user's profile View All Posts By User
DeAdFX
Hazard to Others
***




Posts: 339
Registered: 1-7-2005
Location: Brothel
Member Is Offline

Mood: @%&$ing hardcore baby

[*] posted on 12-4-2006 at 18:41


Well when I took a look at their website http://www.unitedglasstech.com/. It says that they manufacture/repair/modify their own glassware. By reading their website I interrupt that their glassware would fair well against Kimax/Pyrex but having feedback would be apperciated. They also sell other types of glassware like Kimax beakers/clyinders/flasks/etc.



[Edited on 13-4-2006 by DeAdFX]
View user's profile View All Posts By User
MadHatter
International Hazard
*****




Posts: 1332
Registered: 9-7-2004
Location: Maine
Member Is Offline

Mood: Enjoying retirement

[*] posted on 12-4-2006 at 19:00
Question


Send them an e-mail requesting what type of glass they use. They mentioned on the
main page it's not the cheap shit from Mexico or China - big suppliers of Bomex.




From opening of NCIS New Orleans - It goes a BOOM ! BOOM ! BOOM ! MUHAHAHAHAHAHAHA !
View user's profile View All Posts By User
neutrino
International Hazard
*****




Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline

Mood: oscillating

[*] posted on 13-4-2006 at 16:51


If you want to save a few dollars, look at their eBay auctions. They usually give free shipping there.

They say on their eBay auctions "Pyrex glassware". I'm not sure if this means Pyrex-type (borosilicate) or actually Pyrex. Email them for clarification.




View user's profile View All Posts By User
ordenblitz
Hazard to Others
***




Posts: 259
Registered: 18-7-2004
Location: Northwest
Member Is Offline

Mood: Bohr'd

[*] posted on 14-4-2006 at 06:05


My glassware collection is a mix of Pyrex, Kimax, Schott ect. I do not trust low quality glass nor will use it, so I was as skeptical as you when I placed my first order with United. It was for a vacuum distillation adapter which when it arrived, was beyond my expectations. I have ordered two more times with equal satisfaction.

The quality is as good or better than Pyrex brand because the glass is Pyrex but the assembly craftsmanship is better. The glass is Pyrex brand and United mentions this because they buy the flask blanks and other base shapes from Pyrex as well as the loose joints then make the glassware from the pieces. Many makers do the very same thing.

[Edited on 14-4-2006 by ordenblitz]
View user's profile View All Posts By User
evil_lurker
National Hazard
****




Posts: 767
Registered: 12-3-2005
Location: United States of Elbonia
Member Is Offline

Mood: On the wagon again.

[*] posted on 14-4-2006 at 22:04


I've ordered from them several times before and got real pyrex. No air bubbles, flea bites, etc just good quality HEAVY glass.

And their prices... just blows everyone out of the water.

Order from them and you will not be disappointed!
View user's profile View All Posts By User
The_Davster
A pnictogen
*******




Posts: 2861
Registered: 18-11-2003
Member Is Offline

Mood: .

[*] posted on 15-4-2006 at 10:24


Really nice high quality pyrex, prices about as good as it gets for ground glass.

I was not dissapointed.