Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Platinun group metal refining paper
KalleMP
Harmless
*




Posts: 13
Registered: 5-12-2016
Member Is Offline

Mood: No Mood

[*] posted on 25-3-2018 at 10:28
Platinun group metal refining paper


Hi,

While searching for something else I spotted the following paper and thought there might be one or two people here who might be able to glean some tidbit of information from it even if not directly related to the topic.

A review of methods of separation of the platinum-group metals through their chloro-complexes.
Francesco L. Bernardis, Richard A. Grant, David C. Sherrington
doi:10.1016/j.reactfunctpolym.2005.05.011

I found my way to a online PDF via Google at

http://didacforner.net/documentos/A%20review%20of%20methods%...


View user's profile View All Posts By User
aga
Forum Drunkard
*****




Posts: 7030
Registered: 25-3-2014
Member Is Offline


[*] posted on 25-3-2018 at 13:54


Are you a Pt/PGM refiner ?