Gallium in an Al/Hg reduction


Does anyone here know of any patents or has any experience replacing Hg with Gallium in an Al/Hg reduction. Gallium prevents Al from forming an oxide layer and can reduce water to form hydrogen, but would it work in the same fasion as Al/Hg and if so, why is it not more widespread since Gallium is much safer to handle then Hg?
View user's profile View All Posts By User
bio2
National Hazard
****




Posts: 447
Registered: 15-1-2005
Member Is Offline

Mood: No Mood

[*] posted on 24-3-2008 at 08:48


The mercury salt must dissolve the adhering Al oxide as well as inhibit reformation.

Metallic Hg works also albeit very, very slowly.

Will Gallium salts dissolve Al Oxide?
View user's profile View All Posts By User
Fleaker
International Hazard
*****




Posts: 1244
Registered: 19-6-2005
Member Is Offline

Mood: nucleophilic

[*] posted on 24-3-2008 at 11:21


Yes, there is a paper on this effect already. I don't have it handy, but it will work for reductions of -NO2 to NH2 and for several other things.