Suggestions for oil-bath oil?


I'm in need of a cheap bath oil that won't smoke or decompose in the 100-200degC range, preferably something availible at walmart. I could go with a legitimate laboratory oil, but I don't like waiting for shipments.

I've been using ethylene glycol (there's always antifreeze laying around for some reason), but it's really only good if you're outdoors, upwind, and preferably wearing a respirator. Due to the weather, I've got to move everything back indoors for the next couple of weeks. I was thinking of a synthetic motor oil - Anyone care to comment or offer a better suggestion?




If you see me running, try to keep up.
View user's profile View All Posts By User
PainKilla
National Hazard
****




Posts: 306
Registered: 29-4-2004
Member Is Offline

Mood: No Mood

[*] posted on 16-5-2008 at 16:24


Canola oil (or just about any vegetable based oil) works fine for temperatures up to 225*C or so (although I have taken it up to 250*C without any problems).

The only bad? thing about using this is that it makes stuff smell like you're frying food. Hence the bad? :)

[Edited on 16-5-2008 by PainKilla]
View user's profile View All Posts By User
ShadowWarrior4444
Hazard to Others
***




Posts: 226
Registered: 25-4-2008
Member Is Offline

Mood: Sunlight on a pure white wall.

[*] posted on 16-5-2008 at 16:37


Quote:
Originally posted by Intergalactic_Captain
I'm in need of a cheap bath oil that won't smoke or decompose in the 100-200degC range, preferably something availible at walmart. I could go with a legitimate laboratory oil, but I don't like waiting for shipments.

I've been using ethylene glycol (there's always antifreeze laying around for some reason), but it's really only good if you're outdoors, upwind, and preferably wearing a respirator. Due to the weather, I've got to move everything back indoors for the next couple of weeks. I was thinking of a synthetic motor oil - Anyone care to comment or offer a better suggestion?


You should be able to find mineral oil as a laxative in many pharmacies. As it is meant to be taken internally, it is quite pure and can even be used as transformer oil. I believe the decomp temperature for mineral oil is 500C.




A bit of my photography (usually chemisty/physics inspired): ShadowWarrior4444.deviantart.com/gallery
View user's profile Visit user's homepage View All Posts By User
evil_lurker
International Hazard
*****




Posts: 767
Registered: 12-3-2005
Location: United States of Elbonia
Member Is Offline

Mood: On the wagon again.

[*] posted on 16-5-2008 at 17:24


Shadow is dead on.

Get the heavy mineral oil laxative... it'll go at least 225ºC before it even begins to think about smoking.




Not all chemicals are bad. Without chemicals such as hydrogen and oxygen, for example, there would be no way to make water, a vital ingredient in beer.
View user's profile View All Posts By User
Formatik
International Hazard
*****




Posts: 927
Registered: 25-3-2008
Member Is Offline

Mood: equilibrium

[*] posted on 16-5-2008 at 18:05


For heating around 180°C, one can use cold saturated aqueous calcium chloride solution, mineral oil is good around 200°.

Don't forget salt baths can also be used (usually for higher temperatures though), especially those with a low melting eutectic mixture of salts, or melting salts alone. Between 100 and 200°, a salt would be good that melts in that area but does not decompose and should the heating apparatus break, a compound that is not incompatible with the substance being heated .

If you have the CRC handbook you can flip through it and quickly find the melting points of some common solids, and then search to see their hazards and decomposition points.
View user's profile View All Posts By User
Intergalactic_Captain
Hazard to Others
***




Posts: 228
Registered: 4-9-2004
Location: somewhere where i don\'t know where i am
Member Is Offline

Mood: frabjous

[*] posted on 16-5-2008 at 18:46


All right, sounds like I'm going with the laxative...What am I looking at for cost per quantity? I'm guessing it isn't sold by the liter, and I'd like to grab at least 2.



If you see me running, try to keep up.
View user's profile View All Posts By User
MagicJigPipe
International Hazard
*****




Posts: 1554
Registered: 19-9-2007
Location: USA
Member Is Offline

Mood: Suspicious

[*] posted on 16-5-2008 at 18:58


It's VERY expensive for how much you get so recycle it. You might have to buy 2 or 3 bottles. It usually comes in a clear plastic bottle and will simply say, "Mineral Oil" on it.

Like I said, reuse that shit! It's not cheap!

In my area it's about $7 for a pint (473mL). At least it is very pure (USP I believe).

[Edited on 5-16-2008 by MagicJigPipe]




"There must be no barriers to freedom of inquiry ... There is no place for dogma in science. The scientist is free, and must be free to ask any question, to doubt any assertion, to seek for any evidence, to correct any errors. ... We know that the only way to avoid error is to detect it and that the only way to detect it is to be free to inquire. And we know that as long as men are free to ask what they must, free to say what they think, free to think what they will, freedom can never be lost, and science can never regress." -J. Robert Oppenheimer
View user's profile View All Posts By User This user has MSN Messenger
Intergalactic_Captain
Hazard to Others
***




Posts: 228
Registered: 4-9-2004
Location: somewhere where i don\'t know where i am
Member Is Offline

Mood: frabjous

[*] posted on 16-5-2008 at 19:38


That's kind of what I figured, was hoping it would be a bit cheaper though. I guess I'll give canola oil a shot - worst comes to worst I'll just fry up some chicken. No input on motor oil though? I'd imagine it would take the heat, but one thing I've learned over the years is just how counterintuitively most things work out.



If you see me running, try to keep up.
View user's profile View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 16-5-2008 at 19:47


Motor oil smells worse than ass. I don't know what typical smoke point is for various weights, but I would guess regular 10W-30 doesn't need to be very high inside an engine regulated at 80-120C.

Tim




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
MagicJigPipe
International Hazard
*****




Posts: 1554
Registered: 19-9-2007
Location: USA
Member Is Offline

Mood: Suspicious

[*] posted on 16-5-2008 at 21:03


Yeah, I know for a fact synthetic blend 10w30 starts to smoke at around 150*C. At least.

And the smoke is horrible. I would stay away from it. Next time you've been driving for a long time open up your oilcap and look closely. You might see a small amount of smoke coming out. I know I do.




"There must be no barriers to freedom of inquiry ... There is no place for dogma in science. The scientist is free, and must be free to ask any question, to doubt any assertion, to seek for any evidence, to correct any errors. ... We know that the only way to avoid error is to detect it and that the only way to detect it is to be free to inquire. And we know that as long as men are free to ask what they must, free to say what they think, free to think what they will, freedom can never be lost, and science can never regress." -J. Robert Oppenheimer
View user's profile View All Posts By User This user has MSN Messenger
chemrox
International Hazard
*****




Posts: 2953
Registered: 18-1-2007
Location: UTM
Member Is Offline

Mood: LaGrangian

[*] posted on 16-5-2008 at 23:16


I'm using Dot 5 brake fluid -- expensive but doesn't breakdown or smoke at 100-200*C on a humid day, make a shield so your condenser doesn't drip into it and get the condenser off to the side .. otherwisse lots of crackling going on.. no damage though .. annoying. I need to make a rubber pad for my jackstand .. only slightly larger than the space occupied by the feet of my deep fat fryer.. the fryer keeps perfect temp stability!



"When you let the dumbasses vote you end up with populism followed by autocracy and getting back is a bitch." Plato (sort of)
View user's profile View All Posts By User
sonogashira
International Hazard
*****




Posts: 555
Registered: 10-9-2006
Member Is Offline

Mood: No Mood

[*] posted on 17-5-2008 at 04:36


How about using "Vaseline" petroleum jelly? I've never actually tried it but it is very pure, has a very high boiling point and melts around 100F. Might be worthwhile if a high temperature is needed.. Just speculation though.
View user's profile View All Posts By User
MagicJigPipe
International Hazard
*****




Posts: 1554
Registered: 19-9-2007
Location: USA
Member Is Offline

Mood: Suspicious

[*] posted on 17-5-2008 at 10:06


I think it's just as much for what you get. Unless you get generic petrolatum then maybe... I wouldn't heat it with a flame, though. Also, for temperatures up to 150*C, the optical lab I worked in used glycerol.



"There must be no barriers to freedom of inquiry ... There is no place for dogma in science. The scientist is free, and must be free to ask any question, to doubt any assertion, to seek for any evidence, to correct any errors. ... We know that the only way to avoid error is to detect it and that the only way to detect it is to be free to inquire. And we know that as long as men are free to ask what they must, free to say what they think, free to think what they will, freedom can never be lost, and science can never regress." -J. Robert Oppenheimer
View user's profile View All Posts By User This user has MSN Messenger
dann2
International Hazard
*****




Posts: 1523
Registered: 31-1-2007
Member Is Offline

Mood: No Mood

[*] posted on 17-5-2008 at 15:17


Hello,

If you try the vetinary store for laxative (as opposed to human stuff) it will be much cheaper. It is called 'liquid paraffin' in my neck of the woods. Used for pluged up calves etc. Can buy by the gallon. Not too sure if it is the same as mineral oil.

Dann2
View user's profile View All Posts By User
bio2
National Hazard
****




Posts: 447
Registered: 15-1-2005
Member Is Offline

Mood: No Mood

[*] posted on 18-5-2008 at 11:19


Best heating oil for me is that hard, hydrogenated, solid frying "lard" mixture sold unrefrigerated by the kilo, wrapped in paper.

Some versions have a high percentage of cottonseed oil which when hydrogenated has perhaps the highest smoke point of any vegetable oil.

Spill proof when cool, won't smoke at 220 degrees, very cheap, usable for months and makes the lab smell like a french fryer restaurant.

The smell diminishes considerably after it has been used
at high temp for a while.
View user's profile View All Posts By User
Intergalactic_Captain
Hazard to Others
***




Posts: 228
Registered: 4-9-2004
Location: somewhere where i don\'t know where i am
Member Is Offline

Mood: frabjous

[*] posted on 18-5-2008 at 20:30


Cheap wal-mart canola oil seems to boil somewhere around 140 C... I was trying to distill acetic acid from sulfuric and NaOAc and had to stop, the takeoff rate was too slow when trying to keep the oil from boiling. I think I'll try a "crisco" type oil next, though the canola oil held up fine under ~130 C.



If you see me running, try to keep up.
View user's profile View All Posts By User
MagicJigPipe
International Hazard
*****




Posts: 1554
Registered: 19-9-2007
Location: USA
Member Is Offline

Mood: Suspicious

[*] posted on 18-5-2008 at 21:01


Why not just use mineral oil? Why fuck with all of these flammable cooking oils? I don't understand that. Have you ever had a grease fire? It's not fun...

Also, I've heard a mixture of some glycol monoethyl ethers and glycol ethers can be used as a high temperature bath oil. I have access to all of these in bulk quantities (very cheap). Perhaps I shall try them.

EDIT
Also, I take back what I said about mineral oil being very expensive. It's only $2.50 a pint (473mL) for very pure USP grade mineral oil in my area. It's even a little cheaper than that if you get the quart (946mL) size. If you buy a gallon or so (about $18) it should last you a VERY long time if you reuse it. I mean, it's not like it's going to get very dirty as long as you use a clean bath and even if it does it's not that big of a deal.

Use that... I still don't know why nobody has mentioned glycerol. There must be SOME reason why the Lenscrafters optical lab uses it to heat the dye solutions.

[Edited on 5-18-2008 by MagicJigPipe]




"There must be no barriers to freedom of inquiry ... There is no place for dogma in science. The scientist is free, and must be free to ask any question, to doubt any assertion, to seek for any evidence, to correct any errors. ... We know that the only way to avoid error is to detect it and that the only way to detect it is to be free to inquire. And we know that as long as men are free to ask what they must, free to say what they think, free to think what they will, freedom can never be lost, and science can never regress." -J. Robert Oppenheimer
View user's profile View All Posts By User This user has MSN Messenger
evil_lurker
International Hazard
*****




Posts: 767
Registered: 12-3-2005
Location: United States of Elbonia
Member Is Offline

Mood: On the wagon again.

[*] posted on 18-5-2008 at 21:27


Yeah heavy mineral oil laxative works the best.

All the other organic oils such as vegetable and what not have a nasty tendency to polymerize.

Dino based oils smoke like hell.

Brake fluid can take some heat, but it absorbs moisture and gives off dangerous fumes when overheated.




Not all chemicals are bad. Without chemicals such as hydrogen and oxygen, for example, there would be no way to make water, a vital ingredient in beer.
View user's profile View All Posts By User
MagicJigPipe
International Hazard
*****




Posts: 1554
Registered: 19-9-2007
Location: USA
Member Is Offline

Mood: Suspicious

[*] posted on 18-5-2008 at 22:27


Yeah, I think that's what the brake fluid is ... The glycol alkyl ethers and probably some diethylene and triethylene glycol. In fact, I'm sure some of them contain a majority of di-triethylene glycol.

Hmmmmm... I think triethylene glycol might be something to try by itself. It's boiling point is 285*C. It is hygroscopic but I don't think that matters too much as you're going to be heating it anyway. Only thing I can think of is the actual vapors being toxic. Probably something to stay away from now that I think about it. (that means stay away from brake fluid, too)




"There must be no barriers to freedom of inquiry ... There is no place for dogma in science. The scientist is free, and must be free to ask any question, to doubt any assertion, to seek for any evidence, to correct any errors. ... We know that the only way to avoid error is to detect it and that the only way to detect it is to be free to inquire. And we know that as long as men are free to ask what they must, free to say what they think, free to think what they will, freedom can never be lost, and science can never regress." -J. Robert Oppenheimer
View user's profile View All Posts By User This user has MSN Messenger
S.C. Wack
bibliomaster
*****




Posts: 2419
Registered: 7-5-2004
Location: Cornworld, Central USA
Member Is Offline

Mood: Enhanced

[*] posted on 18-5-2008 at 22:42


Grocery store mineral oil will most definitely smoke and burn. It might be rather volatile at the temperature that you want. Depends on the mw. Same with wax. Dudes of yesteryear used wax baths, but I'm not sure that Gulf Wax is so great at higher temperatures.
View user's profile Visit user's homepage View All Posts By User
Formatik
International Hazard
*****




Posts: 927
Registered: 25-3-2008
Member Is Offline

Mood: equilibrium

[*] posted on 19-5-2008 at 01:11


Quote:
Originally posted by MagicJigPipe Use that... I still don't know why nobody has mentioned glycerol. There must be SOME reason why the Lenscrafters optical lab uses it to heat the dye solutions.


I've got a reference (Römpp) that mentions using glycerin for heating baths, they also say its good for heating around 170ºC, they also mention for this purpose: concd. H2SO4 (for heating around 200º, though I wouldn't use this it's too dangerous, hot oil is one thing, hot acid, another); diethylene glycol (for around 245ºC), paraffin (for 250ºC), triethylene glycol (276ºC), and the pentyl ester of silicic acid (360ºC). For temperatures up to 400ºC, mixtures of biphenyl and diphenylether as well as ditolyl ether ("Diphyl"). For temperatures between around 200 to 700ºC, salt baths are employable.

It's also notable mentioning that there are salts which will increase the boiling point of water ("boiling point elevation"), so a salt can be added which gets this effect, one of those is a CaCl2 solution mentioned earlier.

In each case it's important that the flash point of the compounds is not reached and to avoid the harmful gases where they are formed. Baths not using glycols or glycerin are easier to keep anhydrous.
View user's profile View All Posts By User
bio2
National Hazard
****




Posts: 447
Registered: 15-1-2005
Member Is Offline

Mood: No Mood

[*] posted on 19-5-2008 at 13:00


SC Wack is right!

Any of you guys using mineral oil at 200 degrees?

I tried it once years ago and never again. Fumes off badly and veg oil is much
safer at 200 degrees. Wax is just as bad.

Most of these more "unconventional" liquids mentioned have bad odors/fumes and that's
why most people never use them. A closed system is what most of these commercial
heat transfer fluids is intended for.
View user's profile View All Posts By User
evil_lurker
International Hazard
*****




Posts: 767
Registered: 12-3-2005
Location: United States of Elbonia
Member Is Offline

Mood: On the wagon again.

[*] posted on 19-5-2008 at 13:40


The mineral oil must be labeled as heavy which has a higher B.P. than normal "light" mineral oil.

Check out this chart:

http://www.sonneborn.com/literature/INT_white_oils_prop_char...

And yes you can buy it online for like $15 a gallon plus shipping:

http://www.chemistrystore.com/Kaydol35.htm

The product in the above link, Kaydol 35, has a flash point of 224ºC.

[Edited on 19-5-2008 by evil_lurker]




Not all chemicals are bad. Without chemicals such as hydrogen and oxygen, for example, there would be no way to make water, a vital ingredient in beer.
View user's profile View All Posts By User
kalacrow
Harmless
*




Posts: 38
Registered: 23-5-2008
Member Is Offline

Mood: No Mood

[*] posted on 27-5-2008 at 19:24


http://www.ikea.com/us/en/catalog/products/00046786

Very inexpensive if you have an IKEA near you, but I do not know what the bp is for their product (mineral oils differ in their bp). for $4 you can find out :)

Oh one more thing.. I have a friend who is a potter, and they assure me that they can easily make me simple heating mantles (not with wire inside.. like the ones for placing atop heating elements) out of high temp ceramic for pennies, considering they are so "crude", by their standards. Find an example of one online. and see if you can find a friendly potter to avoid the HUGE prices of commercial ceramic heating mantles.


[Edited on 27-5-2008 by kalacrow]
View user's profile View All Posts By User
amrhamed2
Hazard to Self
**




Posts: 60
Registered: 14-12-2007
Member Is Offline

Mood: No Mood

[*] posted on 27-5-2008 at 23:47


a table

ff.png - 36kB