Uranium carbonate leach next steps?


Hi,
i have successfully leached uranium ore using sodium bicarbonate. It glows green under blacklight. My question is, how can i further process the solution. I assume that i should boil it down, but im not sure how to get it to uranium peroxide. I cant find anything about the process and would like some guidance on where i can find documentation, if there is any.

Thanks,
Jackson

image.jpg - 1.1MB
View user's profile View All Posts By User
phlogiston
International Hazard
*****




Posts: 1352
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline

Mood: pyrophoric

[*] posted on 30-12-2018 at 01:15


Have you seen Carl Willis page?

https://carlwillis.wordpress.com/2008/02/20/uranium-chemistr...

Briefly: adjust the pH with acid to the right range and add peroxide.




-----