Author: Subject: Talk to me about V2O5 and toxicity in general
jgourlay
Hazard to Others
***




Posts: 249
Registered: 9-7-2008
Member Is Offline

Mood: No Mood

[*] posted on 11-1-2010 at 12:10
Talk to me about V2O5 and toxicity in general


Gents,

Lately I've become interested in making my own pottery glazes. This pursuit comes thick and heavy with MSDS sheet and toxicity warnings. The base, literally and figuratively, of most of these warnings revolves extensively around "white" and "red" lead because white or red leads form the high-percentage content "base" for about 75% of all pottery glaze recipes.

However, many recipes use a few percent of Vanadium Pentoxide. Now, I've read the MSDS on V2O5 and it looks only slightly less hazardous than a straight chlorine enema. However, the books are not nearly as wound up about V2O5 as they are, say, copper carbonate and chromium compounds. Copper carbonate, btw, is that pretty green string of malachite beads your wife is wearing out to dinner tonight.

Interestingly, there are several commercial glazes that use V2O5. I say "interesting" because the glazes generally come in three classes. 1. "Safe" full stop. 2. "harmful if ingested, safe for food use after firing", and 3. "harmful if ingested, not safe for food use after firing". Most of the recipes containing V2O5 are in the "Safe" category. Now, the warnings indicate you take "safe" with a grain of salt in that 1) they are only safe in liquid, not powdered form and 2) you shouldn't be drinking them. What they mean by "safe" is that your kids can paint with them under supervision and that you don't need to wear gloves or a respirator while using. Additionally, in the recipe books, the recipes listed as "toxic" that use V2O5 are only listed as toxic if they also contain a lead, barium, or if I remember correctly a high percentage strontium compound.

So.....what's the deal with V2O5? Is it dangerous but less dangerous than Copper Carbonate? Is it considered less hazardous by potters because it is less frequently used and in much smaller doses than most other compounds? Ditto questions for the same reasons on Uranium Oxide and praesodymium oxide and the other rare-earth oxides.

Also, anyone know of a good source for V2O5 in sub kilogram quantities?
View user's profile View All Posts By User
per.y.ohlin
Harmless
*




Posts: 27
Registered: 14-11-2009
Member Is Offline

Mood: No Mood

[*] posted on 11-1-2010 at 14:01


The different amounts of compounds likely has a significant effect. If two compounds have a similar toxicity, but one is present in much larger quantities, the compound present in larger quantities will obviously be the one to worry about. Routes of absorption can have an effect as well. Silica is a significant inhalation hazard in a dust form, but it is completely nonhazardous via ingestion or skin absorption. Vanadium pentoxide might be overall about as hazardous as copper carbonate, but in a powder form copper carbonate may be more hazardous.

As for a source, seattle pottery supply seems reasonable. United Nuclear has a similar unit price for less material, but IIRC the shipping costs are horrible.
View user's profile View All Posts By User
jgourlay
Hazard to Others
***




Posts: 249
Registered: 9-7-2008
Member Is Offline

Mood: No Mood

[*] posted on 11-1-2010 at 14:41


Thanks!
View user's profile View All Posts By User
Jor
International Hazard
*****




Posts: 950
Registered: 21-11-2007
Member Is Offline

Mood: No Mood

[*] posted on 12-1-2010 at 02:41


I think it is quite nasty stuff:

http://www.jtbaker.com/msds/englishhtml/v2220.htm
http://msds.chem.ox.ac.uk/VA/vanadium_pentoxide.html
View user's profile View All Posts By User
jgourlay
Hazard to Others
***




Posts: 249
Registered: 9-7-2008
Member Is Offline

Mood: No Mood

[*] posted on 12-1-2010 at 14:02


Thanks for the MSDS. That MSDS is better than the one I printed out the other day.

I've seen several cases like this. HORRIBLY toxic stuff...and yet people seem to have used it pretty successfully over the years without falling over dead.

Not minimizing the hazard...just trying to get a better perspective.
View user's profile View All Posts By User
ScienceSquirrel
International Hazard
*****




Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline

Mood: Dogs are pets but cats are little furry humans with four feet and self determination! :(

[*] posted on 12-1-2010 at 15:44


Realistically if you are using vanadium pentoxide on a micro scale then there should not be a problem as long as you have reasonable containment and gloves etc.
Compared with dimethyl mercury it is not that toxic!
Lead is the major heavy metal in pottery glazes and it is accumulative.
View user's profile View All Posts By User
Sedit
International Hazard
*****




Posts: 1939
Registered: 23-11-2008
Member Is Offline

Mood: Manic Expressive

[*] posted on 12-1-2010 at 20:57


Ok I cant help you with the vanadium pentoxide sorry but I can help you avoid the worse ones out there. Lead oxides are primarly used as a red coloring agent and work very nicely producing a bright colorful red with ease although food safe is out of the question because of acidic foods can leach the lead out. There are some uses as a flux of the lead oxides IIRC but there are many other options there.

Lead as a coloring agent can be done away with using Cadium and most red glazes anymore do just this but Cadium isn't nothing to turn your back on either. There is a safer no toxic although expensive alternative which is Au and its oxides and salts for bright reds and personaly I find this produces the best results of all of them creating a bright but transparent red. Iron can produce earth tone reds but I feel these suck for most applications as you must recrystalize the iron oxides out in order to produce the red color.

If you need any help for glazes I have have taken classes a while back and if needed I could call on much experties help with no problem just PM me and let me know.





Knowledge is useless to useless people...

"I see a lot of patterns in our behavior as a nation that parallel a lot of other historical processes. The fall of Rome, the fall of Germany — the fall of the ruling country, the people who think they can do whatever they want without anybody else's consent. I've seen this story before."~Maynard James Keenan
View user's profile View All Posts By User
JohnWW
International Hazard
*****




Posts: 2849
Registered: 27-7-2004
Location: New Zealand
Member Is Offline

Mood: No Mood

[*] posted on 12-1-2010 at 22:54


There are Fe(III) compounds that can be used as red paint pigments, as in "ferric red" roof paint.
View user's profile View All Posts By User
Sedit
International Hazard
*****




Posts: 1939
Registered: 23-11-2008
Member Is Offline

Mood: Manic Expressive

[*] posted on 12-1-2010 at 23:15


As I stated but these SUCK for red pigments in glazes because the oxides must crystalize out of the melt in microscopic crystals.




Knowledge is useless to useless people...

"I see a lot of patterns in our behavior as a nation that parallel a lot of other historical processes. The fall of Rome, the fall of Germany — the fall of the ruling country, the people who think they can do whatever they want without anybody else's consent. I've seen this story before."~Maynard James Keenan
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 7774
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 14-1-2010 at 11:01


The problem with V2O5 in potteries applications is that it is somewhat volatile, certainly when temperatures are applied, such as common in making of ceramics. So, exposure to V2O5 is quite easy and that is why it is regarded a higher risk chemical in pottery applications.

If you plan to use V2O5 for its intended purpose then you really have to take into account the possibility of vapors of this compound, which will form ultrafine breathable dust when it condenses to a solid again in colder air.
I sometimes use V2O5 for experiments in aqueous solution and in that application I do not think it is really dangerous.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
jgourlay
Hazard to Others
***




Posts: 249
Registered: 9-7-2008
Member Is Offline

Mood: No Mood

[*] posted on 14-1-2010 at 11:57


Woelen, thank you so much for that warning! I have V2O5 on order, and was going to use it until your note. I think I won't use it now. I'm typically not in the shed when I'm firing, but if it will do as you say then I'm going to reconsider. Especially since my little ones are always in the shed, I'm very sensitive to hazards beyond what I can reasonably control.

Maybe in the future if I get one of those fan assemblies that sucks fresh air in from the lid and spits hot air through a fan and out the wall I'll reconsider. But ultrafine condensate all over this small enclosed area isn't going to cut it.
View user's profile View All Posts By User
watson.fawkes
International Hazard
*****




Posts: 2793
Registered: 16-8-2008
Member Is Offline

Mood: No Mood

[*] posted on 14-1-2010 at 15:08


Quote: Originally posted by jgourlay  
Maybe in the future if I get one of those fan assemblies that sucks fresh air in from the lid and spits hot air through a fan and out the wall I'll reconsider. But ultrafine condensate all over this small enclosed area isn't going to cut it.
Take a look at the Orton Ventmaster. The PDF manual on that page has enough information to make your own.

View user's profile View All Posts By User
jgourlay
Hazard to Others
***




Posts: 249
Registered: 9-7-2008
Member Is Offline

Mood: No Mood

[*] posted on 14-1-2010 at 15:10


Man, you guys are such a huge fount of knowledge! Thanks Watson!