How much Platinum in old crooke-xray-tube's anode ?


Hello again, friends, it's been a while ...

I wonder:
There are 2 quite ugly, old crooke-style x-ray-tubes right on my table here,
==> a bigger one (43 cm from end to end), bulb diameter 15.5 cm
==> and a smaller one (28 cm end to end), bulb 8.8 cm

Now the anode are said to be typically made of platinum, see eg.
http://en.wikipedia.org/wiki/Crookes_tube

Quote:

The anode was made of a heavy metal, usually platinum, which generated more x-rays


I would hate to slaughter these relics, but I could use the money for the platinum ...
The anode-diameters are 2 cm and 1 cm ...

Now: Any idea, how thick they might be ?? Back then (1910s and 1920s) the metal was cheaper ...
View user's profile View All Posts By User
entropy51
Gone, but not forgotten
*****




Posts: 1612
Registered: 30-5-2009
Member Is Offline

Mood: Fissile

[*] posted on 20-1-2010 at 06:34


Quote:
I would hate to slaughter these relics, but I could use the money for the platinum ...
It would be a crime to ruin these. Please don't do it.

And it might be tungsten instead of Pt.


[Edited on 20-1-2010 by entropy51]
View user's profile View All Posts By User
chief
International Hazard
*****




Posts: 630
Registered: 19-7-2007
Member Is Offline

Mood: No Mood

[*] posted on 20-1-2010 at 07:29


No tungsten, I've read around, eg.
http://books.google.de/books?id=IXPz7bVR7g0C&pg=PT68&...

I'll try to make photos and find maybe some museum ...

Tungsten wasn't easy enough to work with back then, and Platinum also emitted more efficiently ...
View user's profile View All Posts By User
watson.fawkes
International Hazard
*****




Posts: 2793
Registered: 16-8-2008
Member Is Offline

Mood: No Mood

[*] posted on 20-1-2010 at 17:19


The Pt content puts a floor on the price, but the tubes are possibly more valuable as antiques over that floor. Crookes tubes, I should remind you, are officially 19th century and thus eligible for Victorian Steampunk status, which yields a whole new market population of widely-varying gullibility.
View user's profile View All Posts By User
chief
International Hazard
*****




Posts: 630
Registered: 19-7-2007
Member Is Offline

Mood: No Mood

[*] posted on 21-1-2010 at 13:26


I havent made the photos yet, but: The larger one is even a "self-regulating" one, like described on this site:
http://physics.kenyon.edu/EarlyApparatus/Miscellaneous/X%20R...

[Edited on 21-1-2010 by chief]
View user's profile View All Posts By User
chief
International Hazard
*****




Posts: 630
Registered: 19-7-2007
Member Is Offline

Mood: No Mood

[*] posted on 22-1-2010 at 05:38


Now the pictures:

http://mister-big-busines.de/crooke-xray/index.html

I pay 25 % provision to anyone who can achieve me a good price ~ ! ~

Measurements as above, contact here or via the private-message- function ...
View user's profile View All Posts By User
entropy51
Gone, but not forgotten
*****




Posts: 1612
Registered: 30-5-2009
Member Is Offline

Mood: Fissile

[*] posted on 22-1-2010 at 07:14


The 1917 book "X-rays" by Kaye was a fairly authoritative reference in its time. This book states that the cathode and anode are made of Al. It says that starting in 1897 the anti-cathode is made of Ni with a 1/100 mm thick Pt sheet covering it. Apparently earlier tubes used more Pt, but this became prohibitively expensive. It further states that at that time (1917) tungsten had mostly replaced the Ni/Pt for the anti-cathode.

I think more valuable as antiques than as a source of Pt.

Just discovered the Kaye book online here

[Edited on 22-1-2010 by entropy51]
View user's profile View All Posts By User
chief
International Hazard
*****




Posts: 630
Registered: 19-7-2007
Member Is Offline

Mood: No Mood

[*] posted on 22-1-2010 at 07:35


How old, by that book, do you think these are ? What wattage ? The larger one, with it's 43 cm of length, looks like capable of handling near 100 kV, which at 30 mA would give a heat of 3 kW, much of it at the antikathode (alias "anode" or "target"), and therefore require some serious thickness of the target.

Also the bulb (sized mainly by the heat) with it's 15 cm of diameter is about as large as some old 2000-Watt-incandescent-bulb that I once saw ... ; not a toy, this tube ... !

The 2 outer electrodes really look like aluminum.

The interesting thing is: On google-image-search there are only a few pictures of such tubes, at all !
Any idea about how rare these are and what I can ask for those when offering to a museum ?

[Edited on 22-1-2010 by chief]
View user's profile View All Posts By User
chief
International Hazard
*****




Posts: 630
Registered: 19-7-2007
Member Is Offline

Mood: No Mood

[*] posted on 23-1-2010 at 02:56


The book (link 2 posts above) states plated Ni for cheaper tubes of low output ... ; tungsten on the other hand is brittle, but this target looks "worked", what do you think (?) :
http://mister-big-busines.de/crooke-xray/00448.jpg


[Edited on 1-25-2010 by Polverone]
View user's profile View All Posts By User
chief
International Hazard
*****




Posts: 630
Registered: 19-7-2007
Member Is Offline

Mood: No Mood

[*] posted on 23-1-2010 at 03:18


Here now the downsized images, for the high-res ones go to the gallery
( http://mister-big-busines.de/crooke-xray/ )

































View user's profile View All Posts By User
chief
International Hazard
*****




Posts: 630
Registered: 19-7-2007
Member Is Offline

Mood: No Mood

[*] posted on 24-1-2010 at 04:50


I thought over it: I prefer to sell those, not to destroy them ... ...
How does 500 EUR for both of them sound ?

Simple to operate: Just diminish the vacuum by heating the substances in the side-tubes a bit, and then plainly connect some HV-source with maybe 10-50 mA capability ...

The polychromatic ray is probably good for some basic x-ray-crystallography ... maybe Laue- or even Debye-Scherrer- experiments ...

Also I thought about an x-ray-flashlight: Discharge some Leiden-bottles into the tube, for single pulses of strong radiation ... ...


Maybe I would trade them for something else, like a really nice Laboratory-furnace (multi-kW), or maybe an working electricity-Generator (preferably on Diesel) ...

These things are in east-germany ... as well as a couple of other old tubes ...

[Edited on 24-1-2010 by chief]
View user's profile View All Posts By User
dann2
International Hazard
*****




Posts: 1523
Registered: 31-1-2007
Member Is Offline

Mood: No Mood

[*] posted on 24-1-2010 at 12:45


Hello Chief,

Greetings to East Germany! Original home of the Chlorates Bitterfeld (if I am not mistaken)

While it is not really any of my business, I would be inclined to say that it would be plain WRONG to break up those baby's to get Pt out of them. Try ebay with a reserve?



Cheers,
Dann2
View user's profile View All Posts By User

  Go To Top