hydrogen or carbon monoxide
The left over copper oxide can then be converted to copper metal in the presence of hydrogen or carbon monoxide:
CuO + H2 ? Cu + H2O
CuO + CO ? Cu + CO2
What do they mean presence of hydrogen or carbon monoxide do I add they and how do I make them
|
|
|
entropy51
Gone, but not forgotten
   
Posts: 1612
Registered: 30-5-2009
Member Is Offline
Mood: Fissile
|
|
See page 43 of Chemistry in the Laboratory
For that matter, see all the other pages too!
|
|
|
tictacgold
Harmless
Posts: 5
Registered: 16-8-2009
Member Is Offline
Mood: No Mood
|
|
Hi entropy51
How are you
That pdf file is fantastic.
Thanks very much
|
|
|
entropy51
Gone, but not forgotten
   
Posts: 1612
Registered: 30-5-2009
Member Is Offline
Mood: Fissile
|
|
Probably my favorite chemistry book!
|
|
|
tictacgold
Harmless
Posts: 5
Registered: 16-8-2009
Member Is Offline
Mood: No Mood
|
|
Thanks again entropy51
I have this on my agenda to read this entire file
|
|
|
aonomus
National Hazard
  
Posts: 361
Registered: 18-10-2009
Location: Toronto, Canada
Member Is Offline
Mood: Refluxing
|
|
You can also use carbon powder if you don't have these gasses handy.
|
|
|