Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: What material should be used as a vacuum seal?
AdamAlden
I have a theory about life, the universe and everything.
**




Posts: 82
Registered: 18-3-2016
Location: California
Member Is Offline

Mood: Radioactive

smile.gif posted on 16-2-2019 at 13:08
What material should be used as a vacuum seal?


I need a sheet of a rubber like material to be used between two surfaces to form a vacuum seal. The surface is an acrylic cylinder and two acrylic disks on either side. So the material needs to go between the lip of the cylinder and the disks to seal it when a vacuum is applied.

Does anyone know what kind of material is best? I need to buy it as a sheet and cut it to the right size.'


Also sorry for my previous posts I've been diagnosed with schizoaffective disorder and gone on medication for almost a year and it seems to have helped me out a lot.




I am a buttmeister
View user's profile Visit user's homepage View All Posts By User
Ubya
International Hazard
*****




Posts: 1213
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline

Mood: I'm a maddo scientisto!!!

[*] posted on 16-2-2019 at 13:22


neoprene rubber sheet should work for you




---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make

If you are looking for chemicals check this out: [For Sale]300 chemicals (rare & unusual)
---------------------------------------------------------------------
View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 16-2-2019 at 19:32


Silicone's another good option (get the softer stuff, obviously). Pretty sure you can buy sheets as some sort of kitchen accessory?



Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
Twospoons
International Hazard
*****




Posts: 1201
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline

Mood: A trace of hope...

[*] posted on 17-2-2019 at 12:24


Neoprene is better than silicone. The gas permeability of silicone is surprisingly high. I make a product that uses silicone tube as a gas diffusion membrane. That may or may not matter in your application of course.



Helicopter: "helico" -> spiral, "pter" -> with wings
View user's profile View All Posts By User
SWIM
International Hazard
*****




Posts: 970
Registered: 3-9-2017
Member Is Offline


[*] posted on 17-2-2019 at 16:32


Neoprene is what they used to use as a seal in old-style Virtis lyophilizer flasks , and high vac is the whole point with those babies so it must work well.

If you only need one open end, you might be able to bond the other end on with some monomer based adhesive instead of using a gasket. I know this can be done with plexiglass, but don't know much about acrylic.

This ought to result in a stronger vac chamber if its doable.





View user's profile View All Posts By User
AdamAlden
I have a theory about life, the universe and everything.
**




Posts: 82
Registered: 18-3-2016
Location: California
Member Is Offline

Mood: Radioactive

[*] posted on 17-2-2019 at 17:19


Neoprene looks kind of stiff or tough but it should still make a good seal with some pressure applied. Thanks for advice guys I'll give it a try.



I am a buttmeister
View user's profile Visit user's homepage View All Posts By User
XeonTheMGPony
International Hazard
*****




Posts: 1609
Registered: 5-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 18-2-2019 at 06:11


use a silicone based lube, Vitron is my general go to due to its fairly good chemical compatibility
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3272
Registered: 8-2-2015
Location: UK ... on extended Holiday in Malaysia
Member Is Offline


[*] posted on 18-2-2019 at 08:41


Although silicone rubbers are more porous than natural rubber or many synthetic rubbers,
it is a good choice because - it is cheap and it works.
Chemical resistance is good,
you probably will not notice the porosity unless you are going for high vacuum.

Have you calculated the force on the end disks ?
I worry sometimes when I see YT videos of folks applying vacuum to large thin acrylic disks.




CAUTION : Hobby Chemist, not Professional or even Amateur