How can i purify NH4NO3 fertilizer?


I got some NH4NO3 fertilizer from store to make rocket fuel by mixing it with sugar but the fertilizer seems to mixed with something else as it didn't burned when i tried to ignite the mix, i also tried mixing it with Al powder but it also didn't worked. I tries to recrystallize it but again it doesn't seems to work at all. So can someone tell me how can i get pure NH4NO3 out of that fertilizer.
Thanks in advance.
View user's profile View All Posts By User
morganbw
International Hazard
*****




Posts: 561
Registered: 23-11-2014
Member Is Offline

Mood: No Mood

[*] posted on 5-3-2019 at 01:39


What this gentleman did should be a good start.
After doing as he did it might be a good idea to recrystallize from methanol.
Recystallization of Ammonium Nitrate.
View user's profile View All Posts By User