How would I Extract Iron from Bog Iron


Is it possible to sperarate iron from bog iron without using poisonous CO, I want to get a soluble salt like Iron Acetate or something like that. Thanks for the help

[Edited on 11-8-2019 by Kovoc]
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 5763
Registered: 4-10-2014
Location: Unmoved
Member Is Offline

Mood: Possessor of a tidy and organised lab. Now to mess it up again.

[*] posted on 10-8-2019 at 17:05


Cody did this not long ago. Not one of his yt vids that I actually watched. But you might find some insight there.



View user's profile View All Posts By User
Ubya
International Hazard
*****




Posts: 1213
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline

Mood: I'm a maddo scientisto!!!

[*] posted on 11-8-2019 at 01:09


cody searched bog iron to smelt it, if you just want an iron salt just add the acid you want. bog iron is iron oxyhydroxides, already oxidized, add acetic acid or any acid of your choice, it should dissolve bog iron (essentially it is rust)




---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make

If you are looking for chemicals check this out: [For Sale]300 chemicals (rare & unusual)
---------------------------------------------------------------------
View user's profile View All Posts By User
Kovoc
Harmless
*




Posts: 15
Registered: 2-8-2019
Location: Nova Scotia, Canada
Member Is Offline


[*] posted on 11-8-2019 at 02:31


He wanted to smell a rock?
View user's profile View All Posts By User
icelake
Harmless
*




Posts: 48
Registered: 9-10-2017
Member Is Offline

Mood: No Mood

[*] posted on 11-8-2019 at 02:48


Quote: Originally posted by Kovoc  
He wanted to smell a rock?

https://www.youtube.com/watch?v=YBi5p40UZiU
https://www.youtube.com/watch?v=4A2V6t0qg44
View user's profile View All Posts By User
Ubya
International Hazard
*****




Posts: 1213
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline

Mood: I'm a maddo scientisto!!!

[*] posted on 11-8-2019 at 04:04


Quote: Originally posted by Kovoc  
He wanted to smell a rock?

smelt
/smɛlt/
verb
gerund or present participle: smelting
extract (metal) from its ore by a process involving heating and melting.
"tin smelting"
extract a metal from (ore) by smelting.
"the zinc ores are smelted in Swansea"
https://www.google.com/search?q=smelting&oq=smelting&...





---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make

If you are looking for chemicals check this out: [For Sale]300 chemicals (rare & unusual)
---------------------------------------------------------------------
View user's profile View All Posts By User
Kovoc
Harmless
*




Posts: 15
Registered: 2-8-2019
Location: Nova Scotia, Canada
Member Is Offline


[*] posted on 11-8-2019 at 15:49


I must have read it incorrectly lol
View user's profile View All Posts By User

  Go To Top