Author: Subject: Reaction between Lead (II) Oxide and Manganese (IV) Oxide
SOCl
Harmless
*




Posts: 2
Registered: 12-5-2019
Member Is Offline


[*] posted on 11-9-2019 at 22:31
Reaction between Lead (II) Oxide and Manganese (IV) Oxide


I heated Lead (II) oxide - PbO and Manganese (IV) Oxide - MnO2 in fine powder form to 600-800 deg C (red heat) is resulting in a dark grey powder with a greenish tinge. Does anyone know if these react together ?

I couldn't find anything of that sort in books i have...

I tested it a bit - its is not soluble in water and with HCl it does not give as much chlorine as the manganese dioxide would have ( some chlorine evolves maybe due to some residual MnO2 present). Any further testing ideas is appreciated.

View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 3976
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 11-9-2019 at 22:42


I would guess that you'd get a fused mixture of MnO2, Mn2O3, PbO and PbO2.



Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
SOCl
Harmless
*




Posts: 2
Registered: 12-5-2019
Member Is Offline


[*] posted on 11-9-2019 at 22:51


The mixture never melted visibly on heating.... i had premixed the reactants very well ....it just changed color keeping its powdery form... i was wondering if any plumbate or manganate would form ?
View user's profile View All Posts By User