Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Introducing new amateur chemist
vibbzlab
Hazard to Others
***




Posts: 237
Registered: 6-11-2019
Member Is Offline

Mood: Always curious

[*] posted on 6-11-2019 at 19:47
Introducing new amateur chemist


I am a new amateur chemist. I do run a Youtube channel where I post videos on DIY chemistry projects, demonstrations and academic experiments.i hope everyone will support me

IMG_20190927_141632.jpg - 841kB
View user's profile Visit user's homepage View All Posts By User
vibbzlab
Hazard to Others
***




Posts: 237
Registered: 6-11-2019
Member Is Offline

Mood: Always curious

[*] posted on 6-11-2019 at 20:06


I'm really sorry I am posting this third time. All the other post got glitched. I apologize for that. I think it's ok now
View user's profile Visit user's homepage View All Posts By User
j_sum1
Administrator
********




Posts: 5769
Registered: 4-10-2014
Location: Unmoved
Member Is Offline

Mood: Possessor of a tidy and organised lab. Now to mess it up again.

[*] posted on 6-11-2019 at 20:36


Good to have you here. Sorry about the snuffed account. This happens from time to time and I don't think anyone knows why. My account was wiped a month after joining too.

Anyway, welcome. I look forward to having a few moments to check out your channel.

J.
View user's profile View All Posts By User
vibbzlab
Hazard to Others
***




Posts: 237
Registered: 6-11-2019
Member Is Offline

Mood: Always curious

[*] posted on 6-11-2019 at 20:46


Thank you friend.
This is my channel
https://www.youtube.com/c/vibzzlab
View user's profile Visit user's homepage View All Posts By User
vibbzlab
Hazard to Others
***




Posts: 237
Registered: 6-11-2019
Member Is Offline

Mood: Always curious

[*] posted on 7-11-2019 at 16:18
Got equipment for new lab.


Also got some glassware for the new lab . It was cheap and I got all these for 6usd.
Do you think I should have some specific equipment other than these which are absolutely necessary?

IMG_20191031_072719.jpg - 2MB
View user's profile Visit user's homepage View All Posts By User
Amos
International Hazard
*****




Posts: 1394
Registered: 25-3-2014
Location: Yes
Member Is Offline

Mood: No

[*] posted on 8-11-2019 at 06:48


Invest in a reliable magnetic stir hot plate if you haven't already, and treat it like your one true god from there on. One of these is the cornerstone of any experiment with a good yield. I promise it's worth saving for and paying for early.
View user's profile View All Posts By User
vibbzlab
Hazard to Others
***




Posts: 237
Registered: 6-11-2019
Member Is Offline

Mood: Always curious

[*] posted on 8-11-2019 at 06:58


I have got the condenser. So maybe I should invest for a heating mantle?
View user's profile Visit user's homepage View All Posts By User
Ubya
International Hazard
*****




Posts: 1213
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline

Mood: I'm a maddo scientisto!!!

[*] posted on 8-11-2019 at 08:29


Quote: Originally posted by vibbzlab  
I have got the condenser. So maybe I should invest for a heating mantle?

You can use an oil or water bath, it is not 100% necessary to have a heating mantle





---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make

If you are looking for chemicals check this out: [For Sale]300 chemicals (rare & unusual)
---------------------------------------------------------------------
View user's profile View All Posts By User
vibbzlab
Hazard to Others
***




Posts: 237
Registered: 6-11-2019
Member Is Offline

Mood: Always curious

[*] posted on 8-11-2019 at 08:32


Oh ok let's see what I can do about it.
Thats about heating element.
I will need cabinets to store chemicals now. Since I have got a lot of chemicals, I need to arrange them properly





Amateur chemist. Doctor by profession
Have a small cute home chemistry lab.


Please do check out my lab in YouTube link below

This is my YouTube channel
View user's profile Visit user's homepage View All Posts By User
vibbzlab
Hazard to Others
***




Posts: 237
Registered: 6-11-2019
Member Is Offline

Mood: Always curious

[*] posted on 9-11-2019 at 08:34


Is there alternative to silica crucibles. I actually wanted to do a video on something and it needs a very high temperature




Amateur chemist. Doctor by profession
Have a small cute home chemistry lab.


Please do check out my lab in YouTube link below

This is my YouTube channel
View user's profile Visit user's homepage View All Posts By User
Schmiddy
Harmless
*




Posts: 31
Registered: 6-11-2019
Member Is Offline


[*] posted on 9-11-2019 at 14:45


I checked out the channel, subbed and will be watching some of those testing vids later

I would also suggest you get a hot plate,you can find cheap ones in the 500-1500w range,single or double element with infinite control and you can do an amazing amount with them.

I have a 1000w single element and use it for all my distillations indoors at home, she's a workhorse and I picked it up for $15 at a thrift shop. I use it for everything from ether on up to to Kerosene but mostly water and alcohol.

I can use my boiling flasks directly on the element,with a water bath,oil bath or sand bath.

for most liquid distillations you don't need magnetic stirring,mag stirrers are nice for dissolving powders into liquids and for more complicated reactions like refluxing and distillations that involve powders or non soluble components that need constant stirring to react.

I suggest you get a cheap hot plate first and then concern yourself with a more expensive magnetic stirring heating mantle.
View user's profile View All Posts By User
HydrogenSulphate
Harmless
*




Posts: 34
Registered: 13-10-2019
Member Is Offline

Mood: Caffeinated

[*] posted on 9-11-2019 at 15:36


Welcome, welcome! I, too, am a brand new SciMad member, although I have been lurking around for years.
View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 9-11-2019 at 16:25


Quote: Originally posted by vibbzlab  
Is there alternative to silica crucibles. I actually wanted to do a video on something and it needs a very high temperature


Typically, a stainless steel egg dish/small bowl is a godsend for anything needing a makeshift crucible - it's about $4 for a decent size one and it'll get you past 1000 C without a sweat. Failing that, a soup can will work about three times for temperatures around the melting point of aluminum (after the third, it's almost guaranteed to spring a leak). What's your specific use?

I found my hot plate (with magnetic stirrer) for cheap on LabX - it's good to keep an eye on them in case a good auction comes up.




Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
vibbzlab
Hazard to Others
***




Posts: 237
Registered: 6-11-2019
Member Is Offline

Mood: Always curious

[*] posted on 9-11-2019 at 17:24


I wanted to heat potassium nitrate with carbon to make potassium nitrite.




Amateur chemist. Doctor by profession
Have a small cute home chemistry lab.


Please do check out my lab in YouTube link below

This is my YouTube channel
View user's profile Visit user's homepage View All Posts By User
SWIM
International Hazard
*****




Posts: 970
Registered: 3-9-2017
Member Is Offline


[*] posted on 9-11-2019 at 18:03


You can also use a used automotive oil filter cartridge as a steel crucible.
Just cut the outer shell free of the internals at the base with a hacksaw.

I've put a steel cover on one and piled hot hardwood coals over and around it for hours with no problems at red heat.

I'm sure a good stainless steel bowl like elementcolector1 recommended, would last longer though, and probably contaminate your sample less.

On a small scale a nickel crucible might be a good choice.

You'd need a lot more heat than a Bunsen burner for a bowl or oil filter cartridge I bet.

The most recent thread for making nitrites on here also has a method for reducing the nitrate with zinc in aqueous solution.
It sounds pretty simple, but the poster warned about getting the reaction conditions right to avoid over reduction.




View user's profile View All Posts By User
Texium
Administrator
********




Posts: 3890
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline

Mood: Triturated

[*] posted on 9-11-2019 at 18:24


Quote: Originally posted by SWIM  
You can also use a used automotive oil filter cartridge as a steel crucible.
Just cut the outer shell free of the internals at the base with a hacksaw
Well, now I know what I'm doing next time I change my oil!



Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
vibbzlab
Hazard to Others
***




Posts: 237
Registered: 6-11-2019
Member Is Offline

Mood: Always curious

[*] posted on 9-11-2019 at 19:16


Thank you friends for supporting my works. And about the hot plate I don't know where to get one here. I am from India,I don't find any hotplate cheap here




Amateur chemist. Doctor by profession
Have a small cute home chemistry lab.


Please do check out my lab in YouTube link below

This is my YouTube channel
View user's profile Visit user's homepage View All Posts By User
Steam
Hazard to Others
***




Posts: 237
Registered: 25-3-2014
Location: Minnesota
Member Is Offline

Mood: Triple Point

[*] posted on 10-11-2019 at 17:35


Welcome vibbzlab, have you tried ebay for a hotplate? I got my first two stirring hotplates from that site. If all else fails, every once in a while, one comes up for sale here.



DISCLAIMER: The information in this post is provided for general informational purposes only and may not reflect the current law in your jurisdiction. No information contained in this post should be construed as legal advice from the individual author, nor is it intended to be a substitute for legal counsel on any subject matter. No reader of this post should act or refrain from acting on the basis of any information included in, or accessible through, this post without seeking the appropriate legal or other professional advice on the particular facts and circumstances at issue from a lawyer licensed in the recipient’s state, country or other appropriate licensing jurisdiction.
View user's profile Visit user's homepage View All Posts By User
vibbzlab
Hazard to Others
***




Posts: 237
Registered: 6-11-2019
Member Is Offline

Mood: Always curious

[*] posted on 10-11-2019 at 17:41


I have not tried that yet. I have a round bottom flask with me and some distillation apparatus will it get heated up on a hotplate




Amateur chemist. Doctor by profession
Have a small cute home chemistry lab.


Please do check out my lab in YouTube link below

This is my YouTube channel
View user's profile Visit user's homepage View All Posts By User