[*] posted on 4-12-2019 at 10:09
Ruthenium too good to be true?


https://www.ebay.co.uk/itm/RUTHENIUM-ALLOY-Powder-35g-Very-H...
35g Ru powder for just £22? Seems too good to be true...
View user's profile View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2855
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 4-12-2019 at 10:13


Ru is by far the cheapest of the platinum group metals. This price seems low, but not entirely out of the question



Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
Ubya
International Hazard
*****




Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline

Mood: I'm a maddo scientisto!!!

[*] posted on 4-12-2019 at 11:00


plus it says ALLOY, alloyed with what and in what percentage it's not specified, it could be 90% or 10%, and givem the price, i think it's on the low side

[Edited on 4-12-2019 by Ubya]





---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
View user's profile View All Posts By User
wg48temp9
National Hazard
****




Posts: 789
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline


[*] posted on 4-12-2019 at 11:03


It does not say how much Ru is in the alloy or what the other elements are?



I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
View user's profile View All Posts By User
fff
Harmless
*




Posts: 22
Registered: 20-12-2018
Location: UK
Member Is Offline


[*] posted on 4-12-2019 at 13:22


Same thing with slightly different mass, but also mentioned it's 99.99%...
https://www.ebay.co.uk/itm/RUTHENIUM-Alloy-Powder-45g-Very-H...
View user's profile View All Posts By User
stoichiometric_steve
National Hazard
****




Posts: 827
Registered: 14-12-2005
Member Is Offline

Mood: satyric

[*] posted on 4-12-2019 at 15:13


Quote: Originally posted by wg48temp9  
It does not say how much Ru is in the alloy or what the other elements are?


It's 99.99% powder, the remainder being not powder. So pretty pure powder.
View user's profile View All Posts By User
Ubya
International Hazard
*****




Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline

Mood: I'm a maddo scientisto!!!

[*] posted on 4-12-2019 at 15:17


99.99% pure alloy




---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
View user's profile View All Posts By User
fusso
International Hazard
*****




Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline


[*] posted on 5-12-2019 at 12:37


Just checked the price for ya, Ru is currently $250 or GBP190/ozt. So that does sound suspicious to me, and I doubt it will be 99.99% Ru. If you do want to buy it, proceed with caution and don't expect it to be 99.99% Ru. If it turns out really is, then congrats.



View user's profile View All Posts By User
Mateo_swe
National Hazard
****




Posts: 568
Registered: 24-8-2019
Location: Within EU
Member Is Offline


[*] posted on 7-12-2019 at 11:42


As it clearly says it´s an alloy (a mix), so it´s not pure Ru.
If interested to buy this one should ask the seller what alloy and the %.
View user's profile View All Posts By User
diddi
National Hazard
****




Posts: 723
Registered: 23-9-2014
Location: Victoria, Australia
Member Is Offline

Mood: Fluorescent

[*] posted on 7-12-2019 at 14:59


then what do you do with an alloy? not much good as an element sample, not much good as an Ru source if it is loaded with some unknown contaminant that may be difficult to remove...

not much good at all imo




Beginning construction of periodic table display
View user's profile View All Posts By User
Fleaker
International Hazard
*****




Posts: 1253
Registered: 19-6-2005
Member Is Offline

Mood: nucleophilic

[*] posted on 10-12-2019 at 12:21


Looks like RuO2 to me.

Most commercial Ru metal (sponge) is a light grey powder like the rest of them (barring osmium, that's blue).




Neither flask nor beaker.


"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5139
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 10-12-2019 at 13:50


I wasn't very interested in ruthenium, so I didn't bother much with this thread at the outset.
But I just looked at teh ebay link.
I have "dealt" with that seller before.
Sometimes I got what I paid for.
Sometimes I did not get what I paid for- the material was not "as described".

Proceed with caution + test before you give feedback.
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8106
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 11-12-2019 at 00:15


With this seller you can have good look, but you also can have something completely different.

I have purchased quite a few interesting chemicals from him. To name a few:
- V2O5 --> very good quality material, dissolves completely clear in a solution of NaOH.
- MnO2 --> questionable stuff. Contains a lot of iron. Good enough for energetic thermite-like reactions, but not for anything else.
- NH4ReO4 --> the real thing! pure stuff. I obtained 160 grams for just GBP 40.
- Ru(OH)3 --> not Ru(OH)3, but hydrous RuO2. But it only contains Ru as a metal. A good buy, GBP 20 for 70 grams.
- MoO3 --> impure stuff, contains a lot of brown stuff, does not dissolve completely in solution of NaOH
- WO3 --> very good quality stuff, pure sulphur-yellow material.
- Re --> something completely different, the metal does not dissolve in any acid I have, while Re dissolves in HNO3. With the latter, I received a refund.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net