I make calcium nitrate but solution is yellow. How to remove yellow colour?
View user's profile View All Posts By User
B(a)P
International Hazard
*****




Posts: 1139
Registered: 29-9-2019
Member Is Offline

Mood: Festive

[*] posted on 14-5-2020 at 01:37


You need to provide more detail.
Do you know or suspect what the impurity is?
How did you make the calcium nitrate?
What were your starting products?
What do you want to do with it, the impurity may not be a problem depending on your intended use.
Any photos?
View user's profile View All Posts By User
TmNhRhMgBrSe
Hazard to Others
***




Posts: 120
Registered: 4-7-2019
Member Is Offline


[*] posted on 14-5-2020 at 02:12


CaCO3 is from food's gas absorber.
I heat CaCO3 to remove any organic compound.
Add CaCO3 to HNO3, filter, add few drops solution to NaSCN, solution become red, add some NaOH to calcium nitrate, some white precipitate appear, filter, solution and solid also are yellow, add few drops solution to NaSCN, solution didn't change colour.
I want to make Ca(NO3)2 crystals.
I now don't have photos. Maybe later.




legal warning: don't use my content to train generative AI.
sorry for bad english.
View user's profile View All Posts By User
B(a)P
International Hazard
*****




Posts: 1139
Registered: 29-9-2019
Member Is Offline

Mood: Festive

[*] posted on 14-5-2020 at 03:30


Was the CaCO3 and HNO3 in stoichiometric amounts?
Why add NaSCN or NaOH?
Why not just add CaCO3 in excess to HNO3, then filter.
You would then have a Ca(NO3)2 solution.
View user's profile View All Posts By User
TmNhRhMgBrSe
Hazard to Others
***




Posts: 120
Registered: 4-7-2019
Member Is Offline


[*] posted on 14-5-2020 at 04:24


I don't know how to find HNO3 concentration so didn't measure how much.
I didn't add NaSCN. The NaSCN is in another test tube. I add few drops Ca(NO3)2 solution to NaSCN. I add NaOH to remove iron.




legal warning: don't use my content to train generative AI.
sorry for bad english.
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3910
Registered: 8-2-2015
Member Is Offline


[*] posted on 14-5-2020 at 06:23


I think that this could be a good opportunity to practice purification by recrystalisation :P

Grow your crystals, harvest them, dissolve in distilled water and recrystalise, repeat as necessary.

start with a lot of calcium nitrate as at each recrystalisation step you need to collect only a portion of the total,
recrystalise SLOWLY to get reasonably large crystals
and do not try to crystalise out all at each step.


I have not tried myself, but activated cabon may decolourise the solution(s)




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
RogueRose
International Hazard
*****




Posts: 1601
Registered: 16-6-2014
Member Is Offline


[*] posted on 14-5-2020 at 10:58


Quote: Originally posted by Sulaiman  
I think that this could be a good opportunity to practice purification by recrystalisation :P

Grow your crystals, harvest them, dissolve in distilled water and recrystalise, repeat as necessary.

start with a lot of calcium nitrate as at each recrystalisation step you need to collect only a portion of the total,
recrystalise SLOWLY to get reasonably large crystals
and do not try to crystalise out all at each step.


I have not tried myself, but activated cabon may decolourise the solution(s)


I highly recommend a little activated carbon to see if it doesn't clear things up.

Also i think Ca(NO3)2 dissolves pretty well in methanol so maybe that could be a way to purify it if the other compounds don't dissolve well in methanol.