Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: OTC deep bed gravity microfiltration with minimal pressure drop
mysteriusbhoice
National Hazard
****




Posts: 395
Registered: 27-1-2016
Member Is Offline

Mood: Became chemistry catboy Vtuber Nyaa

[*] posted on 2-9-2020 at 09:55
OTC deep bed gravity microfiltration with minimal pressure drop


https://youtu.be/NXCHw21RGEo
The superabsorbent "scotch brite pad" allows for 2 actions to occur minimizing pressure drop when doing gravity microfiltration.
1. the superabsorbent nature pulls in the water and due to its shape it collects at the bottom thus dripping down thus allowing for great filtration rate even if the filter gets clogged.
2. the effect of multiple layers leading to deep bed filtration also reduces pressure drop thus allowing for decent filtration rate.

This product overall allows you to gain access to a cheap way to perform microfiltration without spending a lot.
View user's profile View All Posts By User
Organikum
resurrected
*****




Posts: 2282
Registered: 12-10-2002
Location: Europe
Member Is Offline

Mood: lonely

[*] posted on 26-7-2022 at 03:03


I found that most decent quality N95 masks do a similar good job in filtration,they can also break emulsions.



Irgendwas is ja immer
View user's profile View All Posts By User
VeritasC&E
Hazard to Others
***




Posts: 169
Registered: 29-1-2018
Member Is Offline

Mood: No Mood

[*] posted on 26-7-2022 at 06:16


Quote: Originally posted by Organikum  
I found that most decent quality N95 masks do a similar good job in filtration,they can also break emulsions.


Do you know what they are made of? is it cellulose? or synthetic fibers? and it what conditions it may contaminate the solvent? They are fairly cheap to get by. I've also wondered about the possibility of using those filters* used to take out microparticles in air (like in vacuum cleaners, or car habitacle air circulation systems, or clean room / lab air filtration systems), but I always figured they probably wouldn't do well / be compatible with solvents for some reason (feared they would be either hydrophobic or have too small pores or that they might be contaminating to the solvent; but hey, fear is the enemy if progress!).

*HEPA Filters

[Edited on 26-7-2022 by VeritasC&E]
View user's profile View All Posts By User
Texium
Administrator
********




Posts: 3879
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline

Mood: Triturated

[*] posted on 26-7-2022 at 08:35


N95 masks are made of polypropylene fibers. Should be resistant to most chemicals.



Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
VeritasC&E
Hazard to Others
***




Posts: 169
Registered: 29-1-2018
Member Is Offline

Mood: No Mood

[*] posted on 27-7-2022 at 14:49


Quote: Originally posted by Texium  
N95 masks are made of polypropylene fibers. Should be resistant to most chemicals.


Thank you for the information! This may save some money in many situations. It also has a fairly large surface area so I guess they may allow for reasonably fast filtration in relation to their small "pore size", plus they are probably more solid than most lab filters. Best used under 40C I would guess.
View user's profile View All Posts By User