I've just started a Potassium Bromate cell with saturated Potassium Bromide solution. I've got a Platinum Anode and a Titanium Cathode. The colours are quite nice!

cell2.jpg - 1.6MB
View user's profile View All Posts By User
Chemgineer
Hazard to Self
**




Posts: 88
Registered: 25-5-2021
Member Is Offline


[*] posted on 4-7-2021 at 07:55


5.8v @ 5amps

You can see the temperature is holding at 52 deg C.

ps. My phone has a Flir thermal imaging camera which is really useful.

flir_20210704T165053.jpg - 1.1MB
View user's profile View All Posts By User
Chemgineer
Hazard to Self
**




Posts: 88
Registered: 25-5-2021
Member Is Offline


[*] posted on 4-7-2021 at 11:03


Ok so I might have to swap the anode to a carbon one... there is a hole through the platinum plating to the titanium underneath at the very tip. I'm guessing this was a fault in the plating surface that it has got into. I've dabbed the damaged area with epoxy for now but have a carbon rod the same diameter if it gets worse.

#Update, switched to the carbon electrode, just means I may have to recrystallise the product so I can filter out the carbon.

[Edited on 4-7-2021 by Chemgineer]
View user's profile View All Posts By User
mysteriusbhoice
National Hazard
****




Posts: 395
Registered: 27-1-2016
Member Is Offline

Mood: Became chemistry catboy Vtuber Nyaa

[*] posted on 4-7-2021 at 12:51


UHHH u know that you should never use a titanium substrate anode in bromate cells as bromide can etch Ti like fluoride can!!
Use graphite or a thick PbO2 anode only.
View user's profile View All Posts By User
Antiswat
International Hazard
*****




Posts: 1621
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline

Mood: dangerously practical

[*] posted on 19-9-2021 at 02:20


if you do this, use a tall container
i lost my MMO to this many years ago haha
no point in using platinum for this, you need fluorine gas to make perbromate
but hey im down to sell you some nifty platinum anodes cheap




~25 drops = 1mL @dH2O viscocity - STP
Truth is ever growing - but without context theres barely any such.

https://en.wikipedia.org/wiki/Solubility_table
http://www.trimen.pl/witek/calculators/stezenia.html
View user's profile View All Posts By User

  Go To Top