Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: AMATEX40
Petn1933
Hazard to Others
***




Posts: 105
Registered: 16-9-2019
Member Is Offline


[*] posted on 8-10-2021 at 06:42
AMATEX40


I had long ago decided to test explosives that were used during World War II and are not currently in use. So I started with amatex.
As you know, amatex came in two forms, 20 and 40, and these numbers indicated the amount of rdx in it.
I tested the Type 40 with an explosive speed of about 7500m / s.
Due to the presence of ammonium nitrate, it must be completely insulated from moisture, so a metal container and waterproof adhesive have been used in this explosive package.
My feeling is that,if there is good protection against moisture, this explosive will have a good performance in public use.

*Each package weighs 1/4 pound.
**5g rdx was used in this test as a booster

***As can be seen in the last picture, the ground was severely affected by the explosion.

5BA664F1-578D-4B78-A52D-C85397533220.jpeg - 371kBA2B92035-A8B9-48D9-95AA-BE63174127A8.jpeg - 400kB2CA6307C-E2DA-4F75-9994-5F0DECE1BB52.jpeg - 702kB8FB553C1-31E8-445B-B3F8-A89F9BB12E19.jpeg - 832kB
View user's profile View All Posts By User
simply RED
Hazard to Others
***




Posts: 204
Registered: 18-8-2005
Location: noitacoL
Member Is Offline

Mood: booM

[*] posted on 8-10-2021 at 06:59


May you give more info on composition and so on...



When logic and proportion have fallen sloppy dead...
View user's profile Visit user's homepage View All Posts By User
Petn1933
Hazard to Others
***




Posts: 105
Registered: 16-9-2019
Member Is Offline


[*] posted on 8-10-2021 at 07:46


You can also search on Google:
TNT:40
RDX:40
Nh4no3:20
Of course, I used 30 grams of ammonium nitrate.
View user's profile View All Posts By User
Nitrosio
Hazard to Self
**




Posts: 57
Registered: 31-3-2018
Member Is Offline

Mood: No Mood

[*] posted on 10-10-2021 at 04:35


3.5 NH4NO3 + C7H5N3O6 = 7 CO + 9.5 H2O + 5 N2
C3H6N6O6 = 3 CO + 3 H2O + 3N2

AN: 38.41% / RDX: 30.45% / TNT: 31.14%

[Edited on 10-10-2021 by Nitrosio]
View user's profile View All Posts By User
caterpillar
National Hazard
****




Posts: 472
Registered: 8-1-2012
Member Is Offline

Mood: No Mood

[*] posted on 12-10-2021 at 13:01


Quote: Originally posted by Nitrosio  
3.5 NH4NO3 + C7H5N3O6 = 7 CO + 9.5 H2O + 5 N2
C3H6N6O6 = 3 CO + 3 H2O + 3N2

AN: 38.41% / RDX: 30.45% / TNT: 31.14%

[Edited on 10-10-2021 by Nitrosio]


CO2 up there, not CO.




Women are more perilous sometimes, than any hi explosive.
View user's profile Visit user's homepage View All Posts By User