Source for Germanium metal ?
For making a silver alloy I need some Ge 'metal'. I got something from ebay 8 years ago, but I need new. I found the Onyxmet has 10g for $27.50 and
some ebay sources have it for a similar price. Is that a reliable price ?
I don't need kilograms, but 20-100g is enough.
|
|
Syn the Sizer
International Hazard
   
Posts: 585
Registered: 12-11-2019
Location: Canada
Member Is Offline
|
|
I would say that isn't a bad price. Looking through my sources it is going at reliable suppliers anywhere from 1200USD-2400USD/kg. For smaller