Manganese sulfate not crystallizing


Hi,

I have purchase (as bulk) Manganese Sulfate from a company that sells bulks chemicals. This comes in a pinkish fine powder.

I have made Manganse Sulfate from batteries (as Der Alte process) and purified as Nurd rage process (making 30% of the solution as Hydroxide, reacting with main solution and filtering)
The solution is then crystallized, which game me the cristals.

But for bought Manganese Sulfate, I cannot get it cristallized and what I ve got now is a brown solution with a brown sludge.

The procees was (it was made 2 times, once with the salts as is was purchased, and once as purified with the nurd rage procees) both gave me the same results.

200ml of dH2O was heated and some manganese sulfate was added till it is saturated at aprox 90°.

It was hot filtered and then it volume was reduced till aprox 50ml without boiling and helped with a fan.

the strong pink solution was left aproximately one week, and as days past the solution got brown with a brown sludge formed at the bottom.

in the nurd rage purification process: after the solution first cools down aprox 30% of it was treated with NaOH, the precipitate (white) was poured into the remaining 70% solution. A pink solution was obtained. the residue in the filter paper was white with a thin layer of brown material (probably oxidation)

1) Does manganese sulphate oxidizes with air?
(in my experience with battery extraction, it form cristalls and does not visible oxidate)

Whats wrong and how can i get cristalls or purify bought manganese sulfate?

thanks,




Go SAFE, because stupidity and bad Luck exist.
View user's profile View All Posts By User
Cathoderay
Harmless
*




Posts: 39
Registered: 29-1-2023
Location: US-Texas
Member Is Offline


[*] posted on 10-3-2023 at 08:49


I think you are a bit unclear.
Sounds like you have two problems, purification and crystallization, and also two different sources of raw material. I gets a bit confusing about what you are referring to at each point.

Have you or have you not been able to do the NurdRage purification and crystallization successfully using the manganese sulfate from batteries?

How can you be sure that the contamination in the bought manganese sulfate is iron?

I have to assume that the brown sludge that appeared while you were waiting a week for it to crystallize was not due to a dust storm (Ha-ha!).
There are three forms of manganese hydroxide, Mn(OH)2 white, MnO(OH)2 and MnO(OH). The last two are brown-black. All three are insoluble or nearly so.
I don't know if an oxidized form would be created fast enough or under the conditions you described.

Unless the material would be effected by heating you should always be able to boil a solution down to the point of getting crystals. As the solution cools more crystals should form.


View user's profile View All Posts By User
RU_KLO
Hazard to Self
**




Posts: 52
Registered: 12-10-2022
Location: Argentina
Member Is Offline


[*] posted on 10-3-2023 at 09:32


1) Have you or have you not been able to do the NurdRage purification and crystallization successfully using the manganese sulfate from batteries?

Yes I have.

2)How can you be sure that the contamination in the bought manganese sulfate is iron?

Im not sure if contamination is Iron. If contaminated, do not know what is the contamination. (I performed Nurd rage process, because was the only one Ive found for purificationof manganese sulfate.
Direct cristallization of bought product did not work.

will try these: Unless the material would be effected by heating you should always be able to boil a solution down to the point of getting crystals. As the solution cools more crystals should form.

(Did not do this earlier because I read that for the cristals to be "purer", they should come out from solution and not from dryness or less mother liquor.)






Go SAFE, because stupidity and bad Luck exist.
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10553
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 10-3-2023 at 12:29


Quote: Originally posted by RU_KLO  

2)How can you be sure that the contamination in the bought manganese sulfate is iron?



Iron and manganese are very often found together and almost certainly in battery MnOx.

But ferric hydroxide and Mn can be separated quite easily. Nurdrage describes a procedure, IIRW...

[Edited on 10-3-2023 by blogfast25]




View user's profile View All Posts By User
Texium
Administrator
********




Posts: 4181
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline

Mood: Triturated

[*] posted on 10-3-2023 at 14:28


Quote: Originally posted by blogfast25  
But ferric hydroxide and Mn can be separated quite easily. Nurdrage describes a procedure, IIRW...
You mean the one he already said that he tried, multiple times in this thread?

@RU_KLO I had a similar experience years ago with some manganese sulfate that I bought on ebay. In my case, it appeared that MnO2 was the contaminant. Industrially, manganese sulfate is made by reduction of MnO2 with SO2. The stuff that I got was brown and there was a lot of insoluble brown sludge when added to water, as you described. It also had a strong odor of SO2 remaining when dissolved in water. I don't remember if I checked for iron. You can see if there is iron contamination easily by adding ferrocyanide. If it is pure manganese, a white/tan precipitate should form, but if there is iron you will clearly see prussian blue.

I had success with mine just by gravity filtering the solution through a couple coffee filters and then boiling down the filtrate. Crystals were slow to form and remained very small, but they were a lovely pale pink.




Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
Cathoderay
Harmless
*




Posts: 39
Registered: 29-1-2023
Location: US-Texas
Member Is Offline


[*] posted on 10-3-2023 at 18:11


RU_KLO, it is true that boiling down will not help purify the substance, but you can crystallize it.
Again, crystallization and purification can be two separate things.
What you might be referring to is Fractional Crystallization. If your air humidity to very high the solution may not evaporate very fast. Dry warm air may help.

Any sludge you have should be able to be removed with filtering with paper with small enough pores. Filter paper with extra small pores is called "Slow", because it is. If there is soluble contamination the filtering will not remove that.

NurdRage had a lot of iron contamination and slow crystallization wouldn't purify it well. He also had a good idea that the contamination was iron, including soluble forms of iron. That may not be your case.

Texium has some good ideas about identifying the contamination. There are probably more analysis that you could do.

Manganese sulfate can crystallize as the monohydrate (pale pink), the pentahydrate (rose) or the tetrahydrate (pink). I'm not sure but it may depend on the temperature. If I understand my reference book, the pentahydrate is most stable between 9 and 26 C, the tetrahydrate between 26 and 27 C and the monohydrate between 57 and 117 C. The anhydrous form is reddish but you can't directly crystallize it from water.
View user's profile View All Posts By User
Jome
Hazard to Others
***




Posts: 153
Registered: 10-6-2004
Location: Soutwest sweden
Member Is Offline

Mood: desiccated

[*] posted on 10-3-2023 at 22:57


I've done the "nurdrage process" several times (though using ceramic MnO2), and it very often turns brown. I think what is happening is that the solution is remaining alkaline, precipitating fine particles of white Mn(OH)2 that are almost invisible as well as fine enough to pass through glass-frit. These are then air-oxidized to brown MnO2. Perhaps SO2 could be bubbled through the solution to get rid of the brown.
View user's profile View All Posts By User This user has MSN Messenger
blogfast25
International Hazard
*****




Posts: 10553
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 11-3-2023 at 05:25


Quote: Originally posted by Jome  
I've done the "nurdrage process" several times (though using ceramic MnO2), and it very often turns brown. I think what is happening is that the solution is remaining alkaline, precipitating fine particles of white Mn(OH)2 that are almost invisible as well as fine enough to pass through glass-frit. These are then air-oxidized to brown MnO2. Perhaps SO2 could be bubbled through the solution to get rid of the brown.


I've used the procedure (which is originally based on some Russian patent) several times, w/o the slightest problem, so I'm surprised you're reporting frequent problems.

The solution should of course be as neutral as possible.




View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10553
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 11-3-2023 at 06:55


Quote: Originally posted by Texium  
You can see if there is iron contamination easily by adding ferrocyanide. If it is pure manganese, a white/tan precipitate should form, but if there is iron you will clearly see prussian blue.



For Fe +III concentrated thiocyanate (KSCN) is more sensitive, I think.




View user's profile View All Posts By User
Jome
Hazard to Others
***




Posts: 153
Registered: 10-6-2004
Location: Soutwest sweden
Member Is Offline

Mood: desiccated

[*] posted on 11-3-2023 at 08:11


By the way, I forgot to add that presence of MnO2 could be checked by adding a pinch of ascorbic acid (vitamin C), the brown MnO2 disappears (reacts within seconds to form a very pale pink Mn2⁺ solution), while Fe-oxides instead form colored solutions.
View user's profile View All Posts By User This user has MSN Messenger
Texium
Administrator
********




Posts: 4181
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline

Mood: Triturated

[*] posted on 11-3-2023 at 11:44


Quote: Originally posted by blogfast25  
Quote: Originally posted by Texium  
You can see if there is iron contamination easily by adding ferrocyanide. If it is pure manganese, a white/tan precipitate should form, but if there is iron you will clearly see prussian blue.

For Fe +III concentrated thiocyanate (KSCN) is more sensitive, I think.
Possibly so, though either should work sufficiently. I personally like the prussian blue test since the color is so different and unmistakable. Ferrocyanide is sensitive to Fe(III) while ferricyanide is sensitive to Fe(II).

Quote: Originally posted by Jome  
By the way, I forgot to add that presence of MnO2 could be checked by adding a pinch of ascorbic acid (vitamin C), the brown MnO2 disappears (reacts within seconds to form a very pale pink Mn2⁺ solution), while Fe-oxides instead form colored solutions.
It depends. If the MnO2 is present in the sample from the beginning, it might be tough calcined stuff that won't readily react with ascorbic acid or other reducing agents.



Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
woelen
Super Administrator
*********




Posts: 7841
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 13-3-2023 at 00:19


If you add a drop, maybe two drops, of dilute H2SO4 to the solution, then it will not oxidize. At high pH, Mn(2+) is very air-sensitive and easily is oxidized to hydrous Mn2O3, or hydrous MnO2. This is the brown sludge you observe. If you add a tiny amount of acid, such that the liquid is somewhat acidic, then the Mn(2+) is quite stable in air. Just adding a drop of acid to e.g. 100 ml of solution is sufficient. Let it stand, so that all brown insoluble matter sinks to the bottom and then decant the clear liquid, which should be nearly colorless (very pale pink). Let this liquid evaporate slowly, and then I expect pale pink crystals.

Do not add too much acid, just a drop, maybe two drops.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
j_sum1
Administrator
********




Posts: 6045
Registered: 4-10-2014
Location: Unmoved
Member Is Offline

Mood: It's chromium time.

[*] posted on 13-3-2023 at 01:38


It's always funny when woelen tells people to drop acid.