Original Destructions


If I'm not mistaken, aside from the "Unconventional Shaped Charges" thread, there isn't one to post the results of shots under particular, and if possible, original circumstances.

And so, I'm kicking things off with the "Love Killer" shot.

A few years ago, my wife gave me a metal heart she had found at a flea market. It was a beautiful piece of metal, weighing about 300-400 grams, quite thick at its center. Instinctively, I immediately thought I could test it with explosives, as I had done countless times before with hard materials like iron, steel, nickel, etc., or rock.

Recently, the opportunity arose to bring this project to life. While visiting friends in the countryside, I set up the device in the hollow of a cut tree trunk to dampen the noise and contain the shrapnel. I also placed an old laptop half a meter away to gauge the size and distribution of the droplets from the copper tube, loaded with 16 grams of EGDN.

The heart was blown to pieces (I only recovered about a third of it), and the laptop was generously splattered with copper droplets.

Now, a crucial question: I told my wife there was no subliminal message in this destruction and that I could easily replace the heart online... BUT I can’t find an equivalent anywhere! So, if anyone knows where to find one, I’d greatly appreciate it. Thanks in advance!

Love Killer .png - 7.3MB
View user's profile View All Posts By User
Metacelsus
International Hazard
*****




Posts: 2542
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline

Mood: Double, double, toil and trouble

[*] posted on 1-1-2025 at 10:13


Lol, if I were the wife I might be . . . *heartbroken*

This pewter heart came up on an Amazon search: https://www.amazon.com/Danforth-Inspirational-Pocket-Valenti...




As below, so above.

My blog: https://denovo.substack.com
View user's profile View All Posts By User
Metallophile
Hazard to Self
**




Posts: 89
Registered: 23-3-2018
Member Is Offline

Mood: No Mood

[*] posted on 1-1-2025 at 11:41


This is definitely an amusing experiment! But it might be good to know, what exactly was the heart made of?
View user's profile View All Posts By User
Sir_Gawain
Hazard to Others
***




Posts: 478
Registered: 12-10-2022
Location: [REDACTED]
Member Is Offline

Mood: Still in 2022

[*] posted on 1-1-2025 at 11:43


Looks like pewter. Try melting a piece, if it is pewter you could just re-cast the heart.



“Alchemy is trying to turn things yellow; chemistry is trying to avoid things turning yellow.” -Tom deP.
View user's profile Visit user's homepage View All Posts By User
pdb
Hazard to Self
**




Posts: 99
Registered: 8-4-2004
Member Is Offline

Mood: No Mood

[*] posted on 15-1-2025 at 05:24
Destruction of a Stainless Steel Cylinder


A few years ago, I had a stainless steel cylinder made (60 mm diameter x 80 mm height) with a central hole (7 mm diameter x 60 mm height) to study the initiation capability of primaries.

Recently, I decided to destroy it... I planned 7 successive detonations: 2 with TNP and then 5 with EDGN. The cavity gradually expanded from 2.3 cm³ to 13 cm³, and the cylinder began to swell after the 4th shot. The final detonation split it into 3 pieces, of which I recovered only one, accounting for 42% of the initial mass. The interior appears layered due to the successive detonations, which progressively cracked the cavity. Carbon deposits, caused by the TNP detonations, are also visible.

Side story: The last detonation cost me a few hundred dollars: a tiny fragment, the size of a grain of sand, pierced the casing of the smartphone, then an electromagnetic shield, and ultimately shattered an integrated circuit.



Inox Cylinder2.jpg - 933kB Smartphone2.jpg - 990kB
View user's profile View All Posts By User
greenlight
National Hazard
****




Posts: 763
Registered: 3-11-2014
Member Is Offline

Mood: Energetic

[*] posted on 15-1-2025 at 09:16


Wow, is the back of the phone plastic or metal?
How thick is that metal shielding in the middle circled area of the phone with the deep dent in it? How deep is the dent or was there penetration too?





View user's profile View All Posts By User
Laboratory of Liptakov
International Hazard
*****




Posts: 1443
Registered: 2-9-2014
Location: Tel Aviv University
Member Is Offline

Mood: old jew

[*] posted on 15-1-2025 at 09:35


Lesson learned:
If any of you have anything valuable or irreplaceable, send it to PBD's workshop.

This man is guaranteed to destroy it....:cool:




Development of primarily - secondary substances: CHP (2015) neutral CHP and Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024) Diper 60 (2025)
View user's profile View All Posts By User
pdb
Hazard to Self
**




Posts: 99
Registered: 8-4-2004
Member Is Offline

Mood: No Mood

[*] posted on 16-1-2025 at 08:06
Euler's Disk


Yes, look what happened to my little nephew's toy! Of course, it works much less well now... :D

Image1.png - 4.1MB
View user's profile View All Posts By User
Plateings
Harmless
*




Posts: 8
Registered: 14-1-2025
Member Is Offline

Mood: Superposition

biggrin.gif posted on 16-1-2025 at 09:10


Quote: Originally posted by pdb  
Yes, look what happened to my little nephew's toy! Of course, it works much less well now... :D




I bet Euler never thought this would be put to such use...:D




"I would rather have questions that can't be answered than answers that can't be questioned." -Richard P. Feynman-
View user's profile View All Posts By User

  Go To Top