[*] posted on 21-4-2011 at 18:56
Sodium - Random Crystal Arrangement


Hopefully someone can help me out with this:

I cut a piece of sodium metal, let it oxidize in air for a short time and then drop it back in the oil. After a short time, random (planar) crystalline formations begin to appear at the fresh cut surface; never fails. They slightly resemble the patterns that are seen on hot-dip galvanized iron, for example.

Below are a couple of pictures and a link to a short video. So how is it that these crystals form and why?





Hmm, well the video looks like shit but here it is: http://www.youtube.com/watch?v=oKrKFZLe8Fg

Tom
View user's profile View All Posts By User
bob800
Hazard to Others
***




Posts: 240
Registered: 28-7-2010
Member Is Offline

Mood: No Mood

[*] posted on 21-4-2011 at 19:21


I know this doesn't really answer your question, but this effect was also noted of woelen's potassium-production write-up:

http://woelen.homescience.net/science/chem/exps/synthesis_K/...

If you scroll 3/4 down the page, you'll see a photo with somewhat similar effects.
View user's profile View All Posts By User
mr.crow
International Hazard
*****




Posts: 884
Registered: 9-9-2009
Location: Canada
Member Is Offline

Mood: 0xFF

[*] posted on 22-4-2011 at 09:37


Very nice, my sodium does that too. This is common with metals. Here is another example with Lead.



Double, double toil and trouble; Fire burn, and caldron bubble
View user's profile View All Posts By User
m1tanker78
International Hazard
*****




Posts: 685
Registered: 5-1-2011
Member Is Offline

Mood: No Mood

[*] posted on 22-4-2011 at 11:40


Thanks for the link mr. crow. That's exactly what I was looking for.