I have a problem with gas coming out of aqua regia
In my laboratory we always dissolve gold with aqua regia. (3:1 conc.HCl + conc.HNO3) And we've found that our fume hood is going to broken.
I seems that the reaction produce red-brown gas (I think it's N2O2) that destroy rubber, metal and pump. I also believe that there are many oxidizing
transparent gas coming out too.
The question is what should I do to protect the fume hood? Is water trap going to work? And how to apply the water trap.
Thanks.
|
|
|
hkparker
International Hazard
   
Posts: 601
Registered: 15-10-2010
Location: California, United States
Member Is Offline
Mood: No Mood
|
|
Yes, aqua regia decomposes to release NO2, NOCl, and Cl2, all of which are very nasty. Work in a fume hood or do the reaction in a container where
you can lead the gasses under water. Be sure to use a suck back trap.
My YouTube Channel
"Nothing is too wonderful to be true if it be consistent with the laws of nature." -Michael Faraday
|
|
|
Paddywhacker
National Hazard
  
Posts: 478
Registered: 28-2-2009
Member Is Offline
Mood: No Mood
|
|
The usual way that I have dealt with acid fumes is to expose concentrated ammonia solution. The ammonia fumes will neutralise the acid fumes. But
you will get visible smoke, and that might alarm some people even though the smoke is much less harmless than the invisible acid fumes.
|
|
|
blogfast25
Thought-provoking Teacher
   
Posts: 10346
Registered: 3-2-2008
Location: Old Blighty
Member Is Offline
Mood: No Mood
|
|
Isn't urea the recommended scrubber solution? I do all these nitric based dissolutions in open air when there's a bit of wind available...
|
|
|
hkparker
International Hazard
   
Posts: 601
Registered: 15-10-2010
Location: California, United States
Member Is Offline
Mood: No Mood
|
|
I use urea crystals for NO2 and it is by far the best. Come to think of it I know it absorbs chlorine as well, but I'm not sure about NOCl.
My YouTube Channel