Here's a question. If one were to leave a small tupperware container of wet lead azide with water just covering the top of the azide, say..., in the a crevice of a stump and left it there all winter, would the freezing temperatures cause the azide to detonate from expansion of ice pressing on the crystals?
View user's profile View All Posts By User
mabuse_
Hazard to Self
**




Posts: 56
Registered: 3-6-2010
Member Is Offline

Mood: No Mood

[*] posted on 7-4-2012 at 11:49


"Look Mummy, I found a geocache!" - Kaboom.
View user's profile View All Posts By User
Fossil
Hazard to Others
***




Posts: 131
Registered: 4-4-2012
Location: Canada
Member Is Offline

Mood: No Mood

[*] posted on 7-4-2012 at 14:53


Most likely not as the cold temperatures should reduce its sensitivity. Don't take my word on this though, since i have never done this before (why would anybody?).
View user's profile View All Posts By User
cyclonitepyro
Harmless
*




Posts: 10
Registered: 1-11-2011
Member Is Offline

Mood: No Mood

[*] posted on 9-4-2012 at 14:58


i don't think cold would matter much for sensitivity with azide. Anyone else have dreams about lead azide being so fine some goes right through coffee filter. Crystals so small when i hit it with a hammer it won't even go off?
View user's profile View All Posts By User
SWIM
International Hazard
*****




Posts: 970
Registered: 3-9-2017
Member Is Offline


[*] posted on 26-10-2021 at 14:25


Lead azide has enough solubility in water that over months the crystals would grow considerably.

Do lead azide crystals develop sufficient internal stress in large sizes to become more sensitive, or even just go off on their own?

(I know this is an old post, but if I'm right this really requires some comment for safety's sake.)


Edit: Dr Mabuse's point is pretty damned important too.
Leaving lead azide where others can find it, especially if its unlabeled, is pretty sketchy.



[Edited on 26-10-2021 by SWIM]




View user's profile View All Posts By User
ManyInterests
National Hazard
****




Posts: 455
Registered: 19-5-2019
Member Is Offline


[*] posted on 26-10-2021 at 17:11


Quote:
Edit: Dr Mabuse's point is pretty damned important too.
Leaving lead azide where others can find it, especially if its unlabeled, is pretty sketchy.


And more importantly, if they even know what lead azide even is. Before getting into energetics I had no idea about any primary explosives and only heard of what a 'number 8 blasting cap' is without even knowing what it is (I know now, but I don't know what the other blasting cap numbers even mean. I.E Number 3 or Number 10, etc).

I'm going to link this incredibly cheesy (but still extremely important) film from the 1950s that educated children to never, ever touch a blasting cap.

https://www.youtube.com/watch?v=Zn8-rbRMV1k

But I am a little curious as to why you'd want to store the stuff like that?

[Edited on 27-10-2021 by ManyInterests]
View user's profile View All Posts By User
MineMan
International Hazard
*****




Posts: 864
Registered: 29-3-2015
Member Is Offline

Mood: No Mood

[*] posted on 27-10-2021 at 23:04


In mining towns in the 1890s literally every day a kid lost an eye or finger
View user's profile View All Posts By User