masses of brown glass bottles!


hi everyone,
Today I bought all these glass bottles yesterday from an art restorer for 60 dollars!
they were filthy and terribly labelled, so at home I cleaned them all with acetone, filtered and labelled them correctly.
in total I bought: 7x 2,5L bottles and 15x 1L bottles. (1 of each missing)
some of the bottles had solvents and alcohols in them
300ml Isopropanol
700ml diethylformamide (smells like fish and i have no use for it, may just give it back to the fish :D, just kidding :P)
600ml acetone
2L ethanol 99%
500ml methanol
500ml methyl ethyl ketone
500ml 80% acetic acid
300ml toluene
the rest were empties.
I have now labelled them. like the labels? :D





picture 1.jpg - 64kBpicture 2.jpg - 53kB




all above information is intellectual property of Pyro. :D
View user's profile View All Posts By User
Hexavalent
International Hazard
*****




Posts: 1564
Registered: 29-12-2011
Location: Wales, UK
Member Is Offline

Mood: Pericyclic

[*] posted on 28-6-2012 at 12:32


Wow! Nice find!

You can never have too many bottles...are they all made of glass? What would have been in all of them originally, or just more of the above solvents?




"Success is going from failure to failure without loss of enthusiasm." Winston Churchill
View user's profile View All Posts By User
Pyro
International Hazard
*****




Posts: 1305
Registered: 6-4-2012
Location: Gent, Belgium
Member Is Offline

Mood: No Mood

[*] posted on 28-6-2012 at 12:46


all the above solvents were in the original bottles, the others contained things like THF!! 2,5 litre bottles of it!
i washed out the empties and let them dry by the heater, got a little high i think :P
like the labels?
yes they are all made of amber glass




all above information is intellectual property of Pyro. :D
View user's profile View All Posts By User
SulfurApothecary
Harmless
*




Posts: 37
Registered: 26-6-2012
Location: Boise
Member Is Offline

Mood: For science!

[*] posted on 28-6-2012 at 13:35


Very nice! Makes me jelous... :D



You can't arrest me, it was for science!
View user's profile View All Posts By User
Pyro
International Hazard
*****




Posts: 1305
Registered: 6-4-2012
Location: Gent, Belgium
Member Is Offline

Mood: No Mood

[*] posted on 28-6-2012 at 14:01


lol, thanks



all above information is intellectual property of Pyro. :D
View user's profile View All Posts By User
blankets
Harmless
*




Posts: 6
Registered: 12-9-2011
Member Is Offline

Mood: No Mood

[*] posted on 28-6-2012 at 15:32


so....... wher did u get the labels or u make?
View user's profile View All Posts By User
dann2
International Hazard
*****




Posts: 1523
Registered: 31-1-2007
Member Is Offline

Mood: No Mood

[*] posted on 28-6-2012 at 15:39



Jammy bastard!

(that not an insult BTW)

Dann2
View user's profile View All Posts By User
Pyro
International Hazard
*****




Posts: 1305
Registered: 6-4-2012
Location: Gent, Belgium
Member Is Offline

Mood: No Mood

[*] posted on 28-6-2012 at 23:58


no prblem.
i made them myself...
heres an attachment

Attachment: container symbols.docx (22kB)
This file has been downloaded 552 times





all above information is intellectual property of Pyro. :D
View user's profile View All Posts By User
jamit
Hazard to Others
***




Posts: 375
Registered: 18-6-2010
Location: Midwest USA
Member Is Offline

Mood: No Mood

[*] posted on 29-6-2012 at 02:10


very nice bottles! And the labels you made, very good! If you don't mind, I'm going to use them with some modification for my labels. thanks again.

View user's profile View All Posts By User
Pyro
International Hazard
*****




Posts: 1305
Registered: 6-4-2012
Location: Gent, Belgium
Member Is Offline

Mood: No Mood

[*] posted on 29-6-2012 at 02:17


yeah, no problem. but can you post me the changes? that way i can fill in what i forgot :P
what you do is copy them on adhesive A4 paper, that way you don't need to fool around with tape




all above information is intellectual property of Pyro. :D
View user's profile View All Posts By User
Pyro
International Hazard
*****




Posts: 1305
Registered: 6-4-2012
Location: Gent, Belgium
Member Is Offline

Mood: No Mood

[*] posted on 2-7-2012 at 03:48


shit!!! I left a full 2,5L bottle full of lacquer that I hadn't transferred to a different container outside, and the sun hit it and it exploded! it literally exploded! there were shards of glass everywhere, and 2,5L of lacquer was lying on deck, slowly trickling into the water!
that's a real pity.