etched beakers and flask


I just received a bunch of beakers and flasks, which is great, but most of them are etched... probably due to potassium hydroxide attacking the glassware.

Is there a problem in using these beakers and flasks for general chemical reactions. Would they contaminate anything? Is the reaction of potassium hydroxide and glass, permanently there but inert so as to not interfere with chemical reactions?

Anyone have this problem with etched glassware and what have you done with them? I have about 25 such beakers and flasks in volumes of 100, 150,250, and 400ml.

View user's profile View All Posts By User
SulfurApothecary
Harmless
*




Posts: 37
Registered: 26-6-2012
Location: Boise
Member Is Offline

Mood: For science!

[*] posted on 28-6-2012 at 22:18


You will probably be fine, don't worry to much about it. As long as they don't have cracks in it you should be good. Though the pretty factor lessens :D



You can't arrest me, it was for science!
View user's profile View All Posts By User
edgecase
Hazard to Self
**




Posts: 65
Registered: 4-11-2011
Location: Ontario, Canada
Member Is Offline

Mood: Viscous

[*] posted on 29-6-2012 at 10:49


I have been wondering if a glassblower could "repair" etched glassware, maybe by heating it so it flows on the surface, but doesn't deform the shape of the vessel? Anyone ever asked a glassblower that?
View user's profile View All Posts By User
inspector071
Hazard to Self
**




Posts: 69
Registered: 20-2-2012
Member Is Offline

Mood: No Mood

[*] posted on 29-6-2012 at 10:53


The glass blower in the glass shop at my university said the only way to fix scratched/etched glass is to indeed heat it to its transition point. I may bring a few of my scratched up filter flasks and see if he can make them look new again.
View user's profile View All Posts By User
chemrox
International Hazard
*****




Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline

Mood: LaGrangian

[*] posted on 29-6-2012 at 11:43


I etched some by cleaning them in an ultrasound with a metal basket and with smaller pieces getting into the larger ones. I've run into something really strange though. I left some glass in the sink for a couple of months. This was resistant to cleaning so it was left in soapy water for another day and maybe some more vigorous treatment. Anyway it got forgotten while some writing was being done. The water got some kind of mold growing in it. As soon as I noticed that I started cleaning. It took four fill and empty cycles and a box of alconox to get rid of the shit and a number of pieces were etched. I'm baffled. The etches look like the mold patterns left by the dead mold after the first new fill of soapy water. I didn't use any strong base in the wash water or anything besides alconox. If anyone else has encountered this please tell me about it. I have not used any flouride compounds the past year at least. In fact I can't recall any, ever. Some of the glassware I picked up off ebay has been "Laboy." Is it softer than other borosillicates?


IMG_0004.JPG - 300kB IMG_0001.JPG - 250kB

[Edited on 29-6-2012 by chemrox]




"When you let the dumbasses vote you end up with populism followed by autocracy and getting back is a bitch." Plato (sort of)
View user's profile View All Posts By User
Fossil
Hazard to Others
***




Posts: 131
Registered: 4-4-2012
Location: Canada
Member Is Offline

Mood: No Mood

[*] posted on 29-6-2012 at 19:23


Try going at your "moldy" with fuming HCl. I use this whenever organic matter gets stuck on my glassware and by organic I mean something with once living cells. Its never failed me.
View user's profile View All Posts By User
Funkerman23
Hazard to Others
***




Posts: 421
Registered: 4-1-2012
Location: Dixie
Member Is Offline

Mood: No Mood

[*] posted on 25-11-2012 at 20:43


Been having some issues with this as well. It's either water scale or somehow the joint grease& hot water did something. I'll try the HCL trick myself and see if that helps. I suspect it is "softer" glass as well. However acetone did nothing to lift the trouble so I can't really say.



" the Modern Chemist is inundated with literature"-Unknown
View user's profile View All Posts By User
Hexavalent
International Hazard
*****




Posts: 1564
Registered: 29-12-2011
Location: Wales, UK
Member Is Offline

Mood: Pericyclic

[*] posted on 26-11-2012 at 08:36


Why have you reported it?

Personally, when I leave glassware to soak in water, I often add a little bleach to the water to avoid the formation of microorganism colonies.




"Success is going from failure to failure without loss of enthusiasm." Winston Churchill
View user's profile View All Posts By User
Dr.Bob
International Hazard
*****




Posts: 2840
Registered: 26-1-2011
Location: USA - NC
Member Is Offline

Mood: Mildly disgruntled scientist

[*] posted on 26-11-2012 at 08:45


Etched glass is not substantially weaker. But I don't like it either. I save those items which are etched for running messy reactions (tar forming, Fl-, or HO- or other etching type reactions) in, with the hope that at least if I ruin them, they were already ugly.

I have never had any luck making glass pretty by annealing it. Repaired etched glass always looks ugly to me after annealing still. I think you have to go hotter than that to remove the etching.

I have also seen goo form in glassware from minerals and mold. I think they cause the mineral to deposit, I agree with the HCl idea. But I have found some glassware that gets dirty just won't come clean, in either a base or acid bath, often it may be etched or something and maybe something ppt on the etched surface and just won't let go. Again, I just save those flasks for messy reactions and don't worry too much.

I also had a beaker with two small cracks in it that I have used for years now, it finally got an open crack on the top, but it still did not break, and the other two cracks near the bottom did not fail even with the added stress. It is a Pyrex brand beaker, and I will say that their stuff is great, and takes abuse in the lab well. That is one area where I don't skimp, I try to only buy Pyrex beakers, at work, by the case they are only slightly more expensive than cheap ones, and they last years longer in the real world.
View user's profile View All Posts By User
watson.fawkes
International Hazard
*****




Posts: 2793
Registered: 16-8-2008
Member Is Offline

Mood: No Mood

[*] posted on 26-11-2012 at 14:28


Quote: Originally posted by Dr.Bob  
I have never had any luck making glass pretty by annealing it. Repaired etched glass always looks ugly to me after annealing still. I think you have to go hotter than that to remove the etching.
That's right. At the annealing temperature, you get relief of internal stress, but the glass doesn't appreciably soften. In order to remove etching or scratching, the glass would have to be mobile enough that surface tension has a chance to act. That might be possible right at or below the softening point, using an extended heat soak, though I don't know for sure.
View user's profile View All Posts By User
Dr.Bob
International Hazard
*****




Posts: 2840
Registered: 26-1-2011
Location: USA - NC
Member Is Offline

Mood: Mildly disgruntled scientist

[*] posted on 26-11-2012 at 19:42


And of course heating above the annealing temp would ruin any joints (24/40 etc), kill calibrations on volumetric glass, and likely ruin stopcock joints and other complex pieces. Not worth the trouble.
View user's profile View All Posts By User
zed
International Hazard
*****




Posts: 2302
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline

Mood: Semi-repentant Sith Lord

[*] posted on 4-12-2012 at 19:41


You could re-polish the glass via motorized buffing, in areas that are accessible. Cerium oxide might work nicely as a buffing agent. The surface of the glass actually flows and seals. This however, does not cause great generalized heating, and the polished glass probably will not require annealing. It is a surface phenomena that was not well understood in the past. I haven't checked lately.

This physical/chemical process is used in lapidary work, to polish most stones. Quartz and Glasses, being among them.