Electrodes


Will gold hold up as an electrode as well as platinum?
View user's profile View All Posts By User
hissingnoise
International Hazard
*****




Posts: 3940
Registered: 26-12-2002
Member Is Offline

Mood: Pulverulescent!

[*] posted on 22-7-2012 at 01:34


The short answer is no! Gold is attacked when used as anode in a chloride electrolyte ─ its chloride appears as a progressively-forming greenish coloured surface coating.

View user's profile View All Posts By User
Swede
Hazard to Others
***




Posts: 491
Registered: 4-9-2008
Member Is Offline

Mood: No Mood

[*] posted on 24-7-2012 at 07:48


There are really only four practical anode materials for (per)chlorates, if that is what you are after.

- graphite
- MMO/DSA
- Lead dioxide
- Platinum

With the latter two making perchlorates as well. There are other materials being investigated. Boron-doped diamond electroplated on a suitable substrate shows great promise but it remains a bit exotic for now.

Just about every other likely material has been tried, and they all fail, either not producing chlorate, crumbling to dust, or both.
View user's profile Visit user's homepage View All Posts By User
Swede
Hazard to Others
***




Posts: 491
Registered: 4-9-2008
Member Is Offline

Mood: No Mood

[*] posted on 24-7-2012 at 08:07


Speaking of boron-doped diamond, has anyone found a source? The one I did find was scary expensive, at $400+ for a "BDD electrode in Teflon 3mm diameter".

Ouch...