Quote: Originally posted by rivetboi  | All 1XXX aluminum alloys are 99% pure. I think the pure wiring alloy you are thinking of is 1199, the high conductivity oxygen free alloy. It is
99.99% aluminum with the remainder being mostly iron, silicon, copper and magnesium.[...]
For the pretty pure but cheap, try getting the 1100 from McMaster-Carr
| The point about 1XXX alloys is true. 99% is perfectly fine for a number of applications. If that's good
enough, then 1100 would do you fine. McMaster carries it; OnlineMetals.com does not stock it, although I'm sure they could get it for you for a price.
The alloy 1350 was the alloy most common in residential, in-wall wiring. 1199 makes good wire, but it's not what was in trade. I'd image that there's
plenty of 1199 used in high-energy physics equipment.
Here's a document on 1XXX alloys from Alcoa that describes their three most common alloys: 1060, 1100, 1350.
|
|
|
S.C. Wack
bibliomaster
   
Posts: 2419
Registered: 7-5-2004
Location: Cornworld, Central USA
Member Is Offline
Mood: Enhanced
|
|
More proof that I literally can't say the simplest, most obvious truths here without "a credible person" saying simple, obvious lies in response. Fuck
this.
[Edited on 2-10-2012 by S.C. Wack]
|
|
|
watson.fawkes
International Hazard
   
Posts: 2793
Registered: 16-8-2008
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by S.C. Wack  |
More proof that I literally can't say the simplest, most obvious truths here without "a credible person" saying simple, obvious lies in response. Fuck
this.
[Edited on 2-10-2012 by S.C. Wack] | Here's the quotation from their own web site, extracted from http://www.onlinemetals.com/aluminumguide.cfm: | Quote: | OnlineMetals.com currently stocks eight alloys of aluminum in various shapes and sizes:
2011 Aluminum (available in Hex, Round)
2024 Aluminum (available in Hex, Plate, Rectangle, Round, Sheet, Square, Tube)
5052 Aluminum (available in Sheet)
6061 Aluminum (available in Angle, Channel, Hex, I-Beam, Pipe, Plate, Rectangle, Rectangle Tube, Round, Sheet, Square, Square Tube, Tube)
6063 Aluminum (available in Angle, Channel, Pipe, Rectangle, Rectangle Tube, Round, Square Tube, Tube)
6101 Aluminum (available in Pipe, Rectangle)
6262 Aluminum (available in Hex, Round)
7075 Aluminum (available in Hex, Plate, Rectangle, Round, Sheet, Square) | Funny, I didn't see any 1XXX alloy
there. So, should I disbelieve their own words?
|
|
|
Eliteforum
International Hazard
   
Posts: 571
Registered: 18-11-2002
Location: United Kingdom
Member Is Offline
Mood: Enjoying the journey
|
|
Ebay. Seriously
All that glitters isn't gold.
|
|
|
Arthur Dent
International Hazard
   
Posts: 546
Registered: 22-10-2010
Member Is Offline
Mood: entropic
|
|
I have literally a drawer-full of aluminium heat sinks from various defunct audio devices and computers, some of them quite old. I wonder if there's a
quick chemical test to determine the purity of the aluminium before grinding down one of these sinks?
Come to think of it, I might also have some of the big electrical "bus" bars described above.
I also have many copper heat sinks, but they scare me since I learned that many of those copper blocks contained some beryllium, and I know that
airborne beryllium dust is WAY nasty. No saw, drill or dremel for those!!!
Robert
--- Art is making something out of nothing and selling it. - Frank Zappa ---
|
|
|
S.C. Wack
bibliomaster
   
Posts: 2419
Registered: 7-5-2004
Location: Cornworld, Central USA
Member Is Offline
Mood: Enhanced
|
|
Anyone else would not be looking for supportive quotes, though, and those who instead go to their front page would notice
Be sure to take a look at our newly-arrived materials:
1100-H14 Aluminum Sheet
at the very top of the product selections, and,
at the aluminum sheet/plate page, 1100 is again at the very top of the product selections, and,
rivetboi's 0.125 sheet which I originally was referring to is second-to-thickest of the .032-.19 offerings, and is available in several sizes (or
custom size), and,
without doing much math, all of their 1100 sheet appears to be cheaper than McMaster-Carr's 1100 products, which go up to 3/8".
And it's been that way since I visited there on 9/22 or 9/23.
And UPS says my package got in town this afternoon.
And my credit card has not yet been billed.
|
|
|
watson.fawkes
International Hazard
   
Posts: 2793
Registered: 16-8-2008
Member Is Offline
Mood: No Mood
|
|
I made an honest mistake about OnlineMetals.com stock based on inconsistent information on their very own web site.
S.C. Wack first calls me a liar: And then claims I'm covering up
after the fact: The lack of good faith that S.C. Wack exhibits in
this interchange is abhorrent to me. In my second post, I quoted the page upon which I had based my original claim, which I am quite certain was my
source, because I pulled from my browser history. Whatever, I suppose, makes him feel better.
|
|
|
cal
Hazard to Self

Posts: 88
Registered: 7-2-2012
Member Is Offline
Mood: No Mood
|
|
Aluminum Wire
Quote: Originally posted by bbartlog  | | If you need high purity Al then aluminum electrical wiring is a good bet. Has to be high purity in order to have an acceptable electrical
conductivity. |
This is correct and some number 4/0 triplex is about 15 dollars for 5 feet. I use this all the time with great results.
[Edited on 7-10-2012 by cal]
|
|
|
Eliteforum
International Hazard
   
Posts: 571
Registered: 18-11-2002
Location: United Kingdom
Member Is Offline
Mood: Enjoying the journey
|
|
Fuck sake, if you need it that bad. Mail me.
All that glitters isn't gold.
|
|
|
Oscilllator
International Hazard
   
Posts: 659
Registered: 8-10-2012
Location: The aqueous layer
Member Is Offline
Mood: No Mood
|
|
"Australian metal powders" is where I get mine from, and although their website doesn't say that they do postage they do. it's $12AUD but I dont know
if they ship overseas. Also I think its about $18AUD/kg.
|
|
|
S.C. Wack
bibliomaster
   
Posts: 2419
Registered: 7-5-2004
Location: Cornworld, Central USA
Member Is Offline
Mood: Enhanced
|
|
Quote: Originally posted by watson.fawkes  | | The lack of good faith that S.C. Wack exhibits in this interchange is abhorrent to me. In my second post, I quoted the page upon which I had based my
original claim, which I am quite certain was my source, because I pulled from my browser history. Whatever, I suppose, makes him feel better.
|
Translation: alleged repeated due diligence failure can't be characterized negatively by lesser beings; tongue the hole of the bullshitters, rather
than be alarmed by unending bullshit.
Bend over and wait, then.
If anyone not looking for cheap unalloyed aluminium does buy nonexistent 1100 from onlinemetals, instead of unwanted rivets from ebay or something, do
look closely for plastic film to peel off before using it.
|
|
|