CuSO4
if i add CuO or CuCO3 or CuCl2 to sulphuric acid will i get CuSO4 ?
|
|
|
Random
International Hazard
   
Posts: 1018
Registered: 7-5-2010
Location: In ur closet
Member Is Offline
Mood: Energetic
|
|
yes if homework question
yet calcined CuO may have hard time reacting and CuCl2 would create a mixture of unwanted ions
|
|
|
Ash96
Harmless
Posts: 9
Registered: 14-11-2012
Member Is Offline
Mood: No Mood
|
|
so i can add CuO or CuCO3 in hot concentrated sulfuric acid right ?
[Edited on 17-11-2012 by Ash96]
|
|
|
Random
International Hazard
   
Posts: 1018
Registered: 7-5-2010
Location: In ur closet
Member Is Offline
Mood: Energetic
|
|
If I wanted to prepare CuSO4 I would use like 35- 50% sulfuric acid at room temp with CuCO3 until no more CuCO3 reacts, then filter and evaporate the
solution
|
|
|
ElectroWin
Hazard to Others
 
Posts: 224
Registered: 5-3-2011
Member Is Offline
Mood: No Mood
|
|
yes, i have done this.
i used hot conc H2SO4 to attack native copper, then make CuSO4, as follows:
H2SO4 + Cu --> CuO + SO2 + H2O
H2SO4 + CuO --> CuSO4 + H2O
the result was a mixture of anhydrous CuSO4 with the monohydrate and CuO.
i purified by dissolving in water and recrystallized; and
the CuO was recycled back to make more CuSO4.
|
|
|
Hexavalent
International Hazard
   
Posts: 1564
Registered: 29-12-2011
Location: Wales, UK
Member Is Offline
Mood: Pericyclic
|
|
Electrolysis of copper in sulfuric acid works well for me when I need more copper sulfate on the fly, as I have a fair amount of technical sulfuric
acid and copper. I also like it due to its ease: I set it up, cover it and leave it sit for a few hours. Et voila, copper sulfate. I usually
recrystallize after making it to maximize purity, and one can get some very nice blue crystals from it.
"Success is going from failure to failure without loss of enthusiasm." Winston Churchill
|
|
|
bfesser
Resident Wikipedian
   
Posts: 2114
Registered: 29-1-2008
Member Is Offline
Mood: No Mood
|
|
Copper(II) oxide will react with concentrated sulfuric acid, generating aqueous copper(II) sulfate, as shown:
CuO<em>(s.)</em> + H<sub>2</sub>SO<sub>4</sub><em>(aq.)</em> →
CuSO<sub>4</sub><em>(aq.)</em> + H<sub>2</sub>O<em>(l.)</em>
Copper(II) carbonate will react with sulfuric acid, generating copper(II) sulfate, as shown:
CuCO<sub>3</sub><em>(s.)</em> + H<sub>2</sub>SO<sub>4</sub><em>(aq.)</em> →
CuSO<sub>4</sub><em>(aq.)</em> + H<sub>2</sub>O<em>(l.)</em> +
CO<sub>2</sub><em>(g.)</em>
Copper(II) chloride may react with concentrated sulfuric acid, liberating hydrogen chloride gas, as shown:
CuCl<sub>2</sub><em>(s.)</em> + H<sub>2</sub>SO<sub>4</sub><em>(aq.)</em> →
CuSO<sub>4</sub><em>(aq.)</em> + 2 HCl<em>(g.)</em>
Avoid using the chloride, as the resulting solution (or first crop of crystals) will invariably contain trace hydrogen and chloride ions, and the
hydrogen chloride gas will hydrate and dissolve your lungs.
|
|
|
bfesser
Resident Wikipedian
   
Posts: 2114
Registered: 29-1-2008
Member Is Offline
Mood: No Mood
|
|
Oh, forgot to mention that concentrated sulfuric acid will dehydrate copper(II) sulfate pentahydrate to anhydrous copper(II) sulfate.
|
|
|