Electrolysis of Copper Sulfate (Electrodes)
I am going to electrolyse copper sulfate to get copper metal and sulfuric acid. First time I used carbon and copper electrodes and it worked fine
except the carbon electrode eroded a lot and I had a significant amount of impurities in the sulfuric acid. This time I have a small piece of gold and
silver. Will the silver work in the electrolysis? I know that iron electrodes definitely don't work because it makes FeSO4. So I don't want to risk
losing the gold so will silver work or will it dissolve or what?
Thanks,
K12
|
|
|
sankalpmittal
Harmless
Posts: 49
Registered: 12-1-2013
Member Is Offline
Mood: Confused....
|
|
Quote: Originally posted by K12Chemistry  | I am going to electrolyse copper sulfate to get copper metal and sulfuric acid. First time I used carbon and copper electrodes and it worked fine
except the carbon electrode eroded a lot and I had a significant amount of impurities in the sulfuric acid. This time I have a small piece of gold and
silver. Will the silver work in the electrolysis? I know that iron electrodes definitely don't work because it makes FeSO4. So I don't want to risk
losing the gold so will silver work or will it dissolve or what?
Thanks,
K12 |
Probably , silver being low in electrochemical series will be discharged first...
|
|
|
IanCaio
Hazard to Self

Posts: 52
Registered: 26-9-2012
Member Is Offline
Mood: No Mood
|
|
I tryied carbon once, but since I used those compass tips I had to change it from time to time, too much trouble, I didnt even finish electrolysing
everything.
Thing is, apart from carbon and platin, theres lead oxide electrodes that would work on this electrolysis, but they are really messy and toxic, so I
recomend you dont even try it.
If theres another alternative, cheaper then platin I would like to know too, because the only reason I'm not trying this experiment again is because I