Graphene Cobalt catalyst at home?


Looks like could do at home. 70c, Near platinum quality ?

http://news.brown.edu/pressreleases/2012/10/catalyst

i like the transducer mixer !
View user's profile Visit user's homepage View All Posts By User
morganism
Hazard to Others
***




Posts: 105
Registered: 8-12-2012
Location: Az.
Member Is Offline

Mood: No Mood

[*] posted on 21-1-2013 at 22:04


maybe increase the surface area of the graphene base , using a magnetic field before mixing in the cobalt?

carbonlett.org

http://carbonlett.org/PublishedPaper/topic_abstract.asp?idx=...

They typically grow sheet on SiC, but hear you can plate any metal under current by just flowing methanol over it.

a straightforward synthesis that requires no explosive hydrogen or methane gas flow. The synthesis is further simplified by using only a liquid carbon source such as methanol. Of over a dozen liquid carbon sources studied, methanol is found to be unique in that it acts as both a carbon/hydrogen source and an inhibitor to amorphous carbon growth. No deposition of amorphous carbon was observed, regardless of vapor pressure, unlike methane and other hydrocarbons. Finally, we describe a protocol to control graphene growth to a single side or selected location on the copper substrate, which is required for most device applications.


Srinivas Gadipelli, Irene Calizo, Jamie Ford, Guangjun Cheng, Angela R. Hight Walker and Taner Yildirim
J. Mater. Chem., 2011,21, 16057-16065

DOI: 10.1039/C1JM12938D


can also use a press mill on poly, then burn the poly off.

another method with a ball mill

http://phys.org/news/2012-03-simple-cheap-mass-produce-graph...



could prob put it straight on paper with silver acetate as a base...
View user's profile Visit user's homepage View All Posts By User
morganism
Hazard to Others
***




Posts: 105
Registered: 8-12-2012
Location: Az.
Member Is Offline

Mood: No Mood

[*] posted on 30-1-2013 at 00:47


using a DVD writer to make graphene electrodes

http://www.gizmag.com/graphene-supercapacitor/21925/